Strenx® Tube 700MLH
Advanced high-strength structural hollow sections
Strenx® Tube 700MLH is an HF-welded cold-formed structural hollow section made of hot-rolled high-strength steel with a minimum yield strength of 700 MPa.
Its high strength combined with naturally stiff form of welded hollow section enables construction of stronger and lighter structures. Strenx® Tube 700MLH meets or exceeds the requirements of EN 10219-3 (2020) and it is CE marked according to EN 1090-2. Typical applications include load-bearing structures in the lifting, handling and transportation segments, especially in conditions that require extremely good toughness.
Strenx® Tube 700MLH is available in circular, square and rectangular shapes. Other shapes and sizes are available upon request.
The maximum length of the tubes is 12-18 meters, depending on the size. Longer or cut-to-length tubes are available upon request.
Hot dip galvanizing Strenx® Tube 700MLH hollow sections may lead to cracking. Please consult SSAB Tech Support prior galvanization.