Strenx® 700 E/F
The high-strength structural steel at 650-700 MPa
Strenx® 700 E/F is a structural steel with a minimum yield strength of 650-700 MPa depending on thickness.
Strenx® 700 E/F meets the requirements of EN 10 025-6 for the S690 grade and thicknesses. Typical applications include demanding load-bearing structures.
Strenx® 700 E (complies with S690QL) is available in plate thicknesses of 4–160 mm, while Strenx® 700 F (complies with S690QL1) is available in plate thicknesses of 4–130 mm.
Benefits include:
- Superior bendability and surface quality
- Weldability with excellent HAZ strength and toughness
- Exceptional consistency within a plate guaranteed by close tolerances
- High impact toughness which provides for good resistance to fractures