SSAB Domex 355ML

SSAB Domex® 355ML

A high-strength heavy plate

SSAB Domex® 355ML is a thermomechanically rolled structural steel plate that provides high strength at low temperatures.

SSAB Domex® 355ML structural steel is easy to weld, bend and process in workshops and on site. Its high strength and good flangeability allow steel structures to be made using thinner steel plates and reduce number of welded joints. Environmentally sound, durable and smart structures are guaranteed using this high-strength, thermomechanically rolled (M) and low temperature (L) tough structural steel grade. SSAB Domex® 355ML meets or exceeds the requirements of S355ML in EN 10025-4.

Dimension Range

SSAB Domex 355ML is available in thicknesses of 6.00-63.00 and in widths up to 3300mm depending on the thickness. More detailed dimensions are provided in the dimension program.

Available Standards

EN 10029

SSAB Domex 355ML

SSAB Domex 355ML

USED FOR
DIMENSIONS
STANDARDS
DATA SHEET
USED FOR

Structural

DIMENSIONS

T: 6 - 63 mm

W: Up to 3300 mm

L: Up to 15000 mm

STANDARDS

EN 10029

DATA SHEET