Proven durability that outlasts the harshest weather.

GreenCoat PLX Pural BT color coated steel is available in regular and matt finishes and offers a wide range of colors inspired by Nordic nature. It uses a patented bio-based coating having Swedish rapeseed oil instead of traditional fossil oil in the paint, which is unique on the market. SSAB holds a worldwide patent for this coating technology (Bio-based Technology, BT).

This product has been developed together with tinsmiths in order to obtain optimum product properties combined with Nordic quality steel and an excellent coating. The result is a unique, premium product for tinsmiths.

GreenCoat PLX Pural BT offers the highest level of durability for standing-seam systems. It is highly formable, even by hand, and has practically no spring-back, which allows for very tight folding.

GreenCoat PLX Pural BT color coated steel offers a coating that is optimized to resist weathering, resulting in excellent UV resistance (Ruv5 for matt appearance) and corrosion classes (RC5+). The slightly structured surface helps to protect against mechanical wear and is easy to handle during manufacturing. GreenCoat PLX Pural BT possesses excellent forming properties enabling very demanding folding even down to -15°C, allowing for year round installation at lower costs.

The reverse side of the sheet is painted with a two-layer grey backside coating.

GreenCoat PLX Pural BT complies with current REACH regulations and is fully chromate-free.

SSAB’s color coated steels are all manufactured according to EN 10169.

 

GreenCoat PLX – "The Roofer’s Choice"

Carl Cross, from Zinc and Copper Roofing Ltd (UK), has installed GreenCoat PLX on a roof and shares his thoughts with us. Take a look at the film."

Product details

GreenCoat coils

GreenCoat PLX Pural BT

GreenCoat PLX Pural BT

MAIN PROPERTIES
COLOR PALETTE
DATA SHEET
MAIN PROPERTIES

Outdoor durability

Mechanical durability

Enhanced formability

Corrosion resistance

Wide color offering

Bio-based Technology (BT)

COLOR PALETTE

  • Snow White
    RR19 / SS0001

  • Quarry Grey
    RR287 / SS0244

  • Anthracite Grey
    RR2H8 / SS0087

  • Mountain Grey
    RR23 / SS0036

  • Nordic Night Black
    RR33 / SS0015

  • Chestnut Brown
    RR887 / SS0435

  • Cottage Red
    RR29 / SS0758

  • Tile Red
    RR750 / SS0760

  • Silver Fir Green
    RR5J3 / SS0975

  • Leaf Green
    RR594 / SS0874

  • Metallic Silver
    RR40 / SS0045

  • Metallic Dark Silver
    RR41 / SS0044

  • Metallic Gold
    RR42 / SS----

  • Metallic Copper
    RR979 / SS0778

DATA SHEET