    General Product Description

    With its corrosion resistant properties, SSAB Weathering 550 minimizes the need for maintenance and corrosion-prevention treatment, contributing significantly to low maintenance costs throughout the product life cycle.

    SSAB Weathering 550 allows for good paint adhesion. The intervals for repainting can be greatly extended compared to plain carbon steel since, if a damage to the paint layer occurs, SSAB Weathering steels have the ability to form a patina layer that minimize corrosion creepage under the paint and inhibits the formation of porous expanding rust.

    In addition to low maintenance costs, the reduced need for corrosion prevention means less use of paint and solvents, making SSAB Weathering 550 an environmentally friendly choice of steel.

    In manufacturing, the steel contributes to excellent productivity thanks to its good formability, toughness and weldability.

    The high-strength of the steel in combination with these properties makes it easier to build lighter and stronger products with increased payload for lower fuel consumption. Typical applications are containers, railway wagons and many others.

    Dimension Range

    SSAB Weathering 550 is available in thickness 3.00-6.10 mm and width up to 1550 mm as coil, slit coil and as cut to length in length up to 15 m, with cut or mill edge.

    Mechanical Properties

    Hide/Show specific columns Edit
    Select columns to display
      Delivery form Thickness
      (mm)
      Test direction
      Yield strength ReH
      (min MPa)
      Tensile strength Rm
      (min MPa)
      Elongation A5
      (min %)
      Min. bending radius 90° bend
      Hot rolled strip 3.00 - 5.99 T 550 600 18 1.0 x t
      Hot rolled strip 6.00 - 6.10 T 550 600 18 1.5 x t
      Compare parameters

      Select one parameter to compare

      Comparison

        Test direction T = Transverse direction.

        Bending properties for both longitudinal and transversal direction.

        Impact Properties

        Hide/Show specific columns Edit
        Select columns to display
          Min. impact energy for longitudinal testing,
          Charpy V 10x10 mm test specimens
          40 J / -20 °C
          Compare parameters

          Select one parameter to compare

          Comparison

            Min. impact energy for longitudinal testing,
            Charpy V 10x10 mm test specimens
            40 J / -20 °C
            Impact testing according to EN ISO 148-1 is performed on thicknesses ≥ 6mm. The specified minimum value corresponds to a full-size specimen.

            Chemical Composition (heat analysis)

            Hide/Show specific columns Edit
            Select columns to display
              C
              (max %)
              Si
              (max %)
              Mn
              (max %)
              P
              (max %)
              Cu
              (max %)
              Cr
              (max %)
              0.10 0.45 0.80 0.12 0.35 0.95
              Compare parameters

              Select one parameter to compare

              Comparison

                The steel is grain refined.

                Additional micro alloying elements Nb, V and Ti can be used.

                Tolerances

                SSAB Weathering is delivered with SSAB Weathering tolerances. Narrower tolerances are available upon request.

                Thickness

                Thickness tolerances correspond to ⅔ of EN 10051 as default value.

                Length and Width

                Width and length tolerances according to SSAB standard which offer narrower tolerances compared to EN 10051.

                For coil and sheet with mill edge, the width tolerances are corresponding to -0/+20 mm.

                For coil and sheet with cut edge, the width tolerances are corresponding to -0/+2 mm.

                Length tolerances only apply for cut to length sheets.

                Shape

                Shape tolerances according to EN 10051.

                Flatness

                Flatness tolerances guarantee a maximum flatness deviation of 3 mm/m in addition to the EN 10051 flatness requirements.

                Flatness guarantees only apply for cut to length sheets.

                Surface Properties

                Hot rolled strip products: According to EN 10163-2 Class A, Subclass 3.

                Delivery Conditions

                Thermomechanically rolled.

                Surface condition

                SSAB Weathering 550 is available with as rolled or pickled surface with mill or cut edge.

                Fabrication and Other Recommendations

                SSAB Weathering 550 is not suited for applications requiring hot working or heat treatments at temperatures above 580°C, since the material then may lose its guaranteed properties.

                The weldability of SSAB Weathering 550 is good. All the conventional fusion welding methods can be used. To obtain the same corrosion resistance in the weld as in the base metal, special filler metals should be used.

                Painting of SSAB weather resistant steel is easy and will result in good paint adhesion. This can further increase the maintenance interval of the component.

                In order to ensure the uniform colour of the patina, all impurities must be cleaned from the steel surface. Organic impurities such as oil or protective greases must be removed by washing. Surface oxidation, oxides or rust can be removed by either shot-blasting or pickling. This will also accelerate the patina formation process. Shot-blasting is not recommended for thicknesses below 4 mm. The surface of clean weathering steel can be pre-patinated by allowing the surface to get wet and dry.

                For information concerning fabrication, see SSAB´s brochures on www.ssab.com or consult Tech Support.

                Appropriate health and safety precautions must be taken when bending, welding, cutting, grinding or otherwise working on the products.

                Contact Information