SSAB Domex® 460ML

Download data sheet

General Product Description

SSAB Domex 460ML is a thermomechanically rolled structural steel plate that provides high strength at low temperatures. SSAB Domex 460ML meets or exceeds the requirements of S460ML in EN 10025-4.

Dimension Range

SSAB Domex 460ML is available in thicknesses of 8.00-63.00 mm and in widths up to 3300 mm depending on the thickness. More detailed dimensions are provided in the dimension program.

Mechanical Properties

Thickness
(mmin)
Thickness
(mmin)
8.00 - 16.000.315 - 0.6299
Yield strength ReH
(min MPa)
460
Tensile strength Rm
(MPa)
540 - 720
Elongation A5
(min %)
17
Thickness
(mmin)
Thickness
(mmin)
16.01 - 40.000.6303 - 1.575
Yield strength ReH
(min MPa)
440
Tensile strength Rm
(MPa)
540 - 720
Elongation A5
(min %)
17
Thickness
(mmin)
Thickness
(mmin)
40.01 - 63.001.575 - 2.480
Yield strength ReH
(min MPa)
430
Tensile strength Rm
(MPa)
530 - 710
Elongation A5
(min %)
17

The tensile test is made transverse to the rolling direction in compliance with EN 10025-4.

Impact Properties

Min. impact energy for longitudinal testing,
Charpy V 10x10 mm test specimens
Min. impact energy for longitudinal testing,
Charpy V 10x10 mm test specimens
40 J / -60 °C 1)

The impact test is made longitudinally to the rolling direction in compliance with EN 10025-4.

1) For thicknesses above 50.00 mm 27J/-50°C.

Chemical Composition (heat analysis)

C
(max %)
C
(max %)
0.14
Si
(max %)
0.50
Mn
(max %)
1.70
P
(max %)
0.020
S
(max %)
0.015
Al
(min %)
0.02
Nb
(max %)
0.05
V
(max %)
0.10
Ti
(max %)
0.05

Carbon Equivalent

Thickness (mmin)
Thickness (mmin)
CET (max %)
8.00 - 63.000.315 - 2.480
0.31
Thickness (mmin)
Thickness (mmin)
CEV (max %)
8.00 - 63.000.315 - 2.480
0.43

 

Tolerances

Thickness

SSAB Domex ML products are delivered with tolerances that correspond to ¾ of EN 10029 Class A as default value.

Length and Width

Width tolerances -0/+4-10 mm depending on the thickness. Length tolerances -0/+15-75 mm depending on length.

Shape

Tolerances according to EN 10029.

Flatness

Maximum flatness deviation 6 mm/m as plate.

Surface Properties

According to EN 10163-2 Class A, Subclass 3.

Delivery Conditions

Thermomechanically rolled (M).

Fabrication and Other Recommendations

Minimum inner bending radius is 1.0 x t transverse to the rolling direction and 1.5 x t longitudinal to the rolling direction up to max 20mm in thickness.

For information concerning fabrication, see SSAB´s brochures on www.ssab.com or consult Tech Support.

Appropriate health and safety precautions must be taken when bending, welding, cutting, grinding or otherwise working on the products.

Contact Information

www.ssab.com/contact 
Copyright 2026