COR-TEN® B Tube

Download data sheet

Select Language

Get datasheet by email
Close

Get datasheet by email

    General Product Description

    COR-TEN® B Tube is structural hollow section with anti-corrosive properties, which minimize the need for maintenance and corrosion-prevention treatment.

    It is available in circular, rectangular, square and special shapes. Customized shapes and other tailoring options are available upon request. It is typically used in advanced engineering and construction where corrosion resistance is important. It meets the standard requirements of EN 10025-5 and EN 10219 and is CE marked.

    COR-TEN® B Tube is manufactured by cold forming and high frequency welding from clean, high quality environmentally friendly steel by modern and efficient tube lines.

    Dimension Range

    COR-TEN® B Tube is available at circular, square and rectangular shapes.

    Hide/Show specific columns Edit
    Select columns to display
      Shapes Dimensions
      Circular (mm) 42.4 - 323.9
      Square (mm) 40x40 - 300x300
      Rectangular (mm) 50x30 - 400x200
      Wall thickness (mm) 2.0 - 12.5
      Mill length (mm) 6000/12 000 mm
      Compare parameters

      Select one parameter to compare

      Comparison

        Shapes
        Circular (mm)
        Dimensions
        42.4 - 323.9
        Shapes
        Square (mm)
        Dimensions
        40x40 - 300x300
        Shapes
        Rectangular (mm)
        Dimensions
        50x30 - 400x200
        Shapes
        Wall thickness (mm)
        Dimensions
        2.0 - 12.5
        Shapes
        Mill length (mm)
        Dimensions
        6000/12 000 mm

        Other shapes, sizes and lengths are available upon request.

        Circular Dimensions

        Hide/Show specific columns Edit
        Select columns to display
          Outer diameter (mm) 2.0 mm (kg/m) 2.5 mm (kg/m) 3.0 mm (kg/m) 4.0 mm (kg/m) 5.0 mm (kg/m) 6.0 mm (kg/m) 8.0 mm (kg/m) 10.0 mm (kg/m) 12.5 mm (kg/m)
          42.4 1.99 2.46 2.91 3.79
          48.3 2.28 2.82 3.35 4.37
          60.3 2.88 3.56 4.24 5.55 6.82
          76.1 3.65 4.54 5.41 7.11 8.77
          88.9 5.33 6.36 8.38 10.4 12.3
          101.6 6.11 7.29 9.63 11.9 14.2
          108.0 6.50 7.77 10.3 12.7 15.1
          114 6.89 8.23 10.9 13.5 16.0
          127.0 7.68 9.17 12.1 15.0 17.9
          139.7 13.4 16.6 19.8 26.0 32.0
          168.3 16.2 20.1 24.0 31.6 39.0
          193.7 18.7 23.3 27.8 36.6 45.3 55.9
          219.1 21.2 26.4 31.5 41.7 51.6 63.7
          273.0 26.5 33.1 39.5 52.3 64.9 80.3
          323.9 39.3 47.0 62.3 77.4 96.0
          Compare parameters

          Select one parameter to compare

          Comparison

            Square Dimensions

            Hide/Show specific columns Edit
            Select columns to display
              Height x Width (mm) 2.0 mm (kg/m) 2.5 mm (kg/m) 3.0 mm (kg/m) 4.0 mm (kg/m) 5.0 mm (kg/m) 6.0 mm (kg/m) 8.0 mm (kg/m) 10.0 mm (kg/m) 12.5 mm (kg/m)
              40 x 40 2.31 2.82 3.30 4.20
              50 x 50 2.93 3.60 4.25 5.45 6.56
              60 x 60 3.56 4.39 5.19 6.71 8.13
              70 x 70 5.17 6.13 7.97 9.70
              80 x 80 5.96 7.07 9.22 11.3 13.2
              90 x 90 6.74 8.01 10.5 12.8 15.1
              100 x 100 7.53 8.96 11.7 14.4 17.0 21.4
              120 x 120 14.3 17.6 20.8 26.4 31.8
              140 x 140 16.8 20.7 24.5 31.4 38.1
              150 x 150 18.0 22.3 26.4 34.0 41.3 48.7
              160 x 160 19.3 23.8 28.3 36.5 44.4 52.6
              180 x 180 27.0 32.1 41.5 50.7 60.5
              200 x 200 30.1 35.8 46.5 57.0 68.3
              220 x 220 39.6 51.5 63.2 76.2
              250 x 250 45.2 59.1 72.7 88.0
              300 x 300 54.7 71.6 88.4 108
              Compare parameters

              Select one parameter to compare

              Comparison

                Rectangular Dimensions

                Hide/Show specific columns Edit
                Select columns to display
                  Height x Width (mm) 2.0 mm (kg/m) 2.5 mm (kg/m) 3.0 mm (kg/m) 4.0 mm (kg/m) 5.0 mm (kg/m) 6.0 mm (kg/m) 8.0 mm (kg/m) 10.0 mm (kg/m) 12.5 mm (kg/m)
                  50 x 30 2.31 2.82 3.30 4.20
                  60 x 40 2.93 3.60 4.25 5.45 6.56
                  80 x 40 3.56 4.39 5.19 6.71 8.13
                  80 x 60 5.17 6.13 7.97 9.70
                  100 x 40 5.17 6.13 7.97 9.70
                  100 x 50 5.6 6.60 8.59 10.5 12.3
                  100 x 60 5.95 7.07 9.22 11.3 13.2
                  100 x 80 6.74 8.01 10.5 12.8 15.1
                  120 x 60 6.74 8.01 10.5 12.8 15.1
                  120 x 80 7.53 8.96 11.7 14.4 17.0 21.4 25.6
                  140 x 60 11.7 14.4 17.0
                  140 x 80 13.0 16.0 18.9
                  150 x 50 11.7 14.4 17.0
                  150 x 100 14.9 18.3 21.7 27.7 33.4
                  160 x 80 14.3 17.6 20.8 26.4 31.8
                  180 x 100 16.8 20.7 24.5 31.4 38.1
                  200 x 100 18.0 22.3 26.4 34.0 41.3 48.7
                  200 x 120 23.8 28.3 36.5 44.4 52.6
                  220 x 120 25.4 30.2 39.0 47.5
                  250 x 100 26.2 31.1 40.2 49.1
                  250 x 150 30.1 35.8 46.5 57.0 68.3
                  260 x 180 39.6 51.5 63.2
                  300 x 100 30.1 35.8 46.5 57.0 68.3
                  300 x 150 40.5 52.8 64.8 78.1
                  300 x 200 45.2 59.1 72.7 88.0
                  400 x 200 54.7 71.6 88.4 108
                  Compare parameters

                  Select one parameter to compare

                  Comparison

                    Mechanical Properties

                    Hide/Show specific columns Edit
                    Select columns to display
                      Yield strength Rp0.2
                      (min MPa)
                      Tensile strength Rm
                      (MPa)
                      Elongation A5
                      (min %)
                      Charpy-V -20°C 10x10 mm test specimen 1)
                      (J)
                      355 510 - 630 20 27
                      Compare parameters

                      Select one parameter to compare

                      Comparison

                        Mechanical properties meet the requirements of S355J2W, EN 10025-5.

                        The mechanical properties for rectangular hollow sections are tested by SSAB on the longer side of the cross section according to EN 10219.

                        1) Impact testing according to EN ISO 148-1 is performed on thicknesses ≥ 6mm. The specified minimum value corresponds to a full-size specimen.

                        Chemical Composition (ladle analysis)

                        Hide/Show specific columns Edit
                        Select columns to display
                          C
                          (max %)
                          Si
                          (%)
                          Mn
                          (%)
                          P
                          (max %)
                          S
                          (max %)
                          Altot
                          (%)
                          Cr
                          (%)
                          Cu
                          (%)
                          0.16 0.30 - 0.50 0.80 - 1.25 0.030 0.030 0.020 - 0.10 0.40 - 0.65 0.25 - 0.40
                          Compare parameters

                          Select one parameter to compare

                          Comparison

                            Chemical composition meets the requirements of S355J2W, EN 10025-5.

                            The steel is aluminium-killed.

                            Carbon Equivalent

                            Hide/Show specific columns Edit
                            Select columns to display
                              Wall Thickness (mm) 2.0 - 12.5
                              CEV (max %) 0.50
                              Compare parameters

                              Select one parameter to compare

                              Comparison

                                Wall Thickness (mm)
                                CEV (max %)
                                2.0 - 12.5
                                0.50

                                CEV value meet the requirements of S355J2W, EN 10025-5.

                                Tolerances

                                Tolerance Circular

                                Hide/Show specific columns Edit
                                Select columns to display
                                  Characteristic Circular hollow sections
                                  Tolerances meet or exceed the requirements of EN 10219
                                  Outside diameter (D) (1 ±1%, with a minimum of ±0.5 mm and a maximum of ±10 mm
                                  Out-of-roundness 2%, when D/T ≤ 100
                                  Thickness (T) When D ≤ 323.9 mm: -5%/+10%, with a minimum of ±0.2 mm and maximum ±0.5 mm
                                  When 355.6 ≤ D ≤ 406.4 mm : ±10%, when T ≤ 5 mm / ±0.5 mm, when T > 5 mm
                                  When D > 406.4 mm : ±10%, with a maximum of ±2 mm
                                  Straightness 0.20% of total length and 3 mm over any 1 m length
                                  Mass per unit length Individual tube: ±6%
                                  Mill length 0/+50 mm, 6000 ≤ L ≤ 18000 mm (standard lengths 6000 & 12000 mm)
                                  Exact length Agreed at the time of enquiry and order
                                  Compare parameters

                                  Select one parameter to compare

                                  Comparison

                                    Characteristic
                                    Outside diameter (D) (1
                                    Circular hollow sections
                                    Tolerances meet or exceed the requirements of EN 10219
                                    ±1%, with a minimum of ±0.5 mm and a maximum of ±10 mm
                                    Characteristic
                                    Out-of-roundness
                                    Circular hollow sections
                                    Tolerances meet or exceed the requirements of EN 10219
                                    2%, when D/T ≤ 100
                                    Characteristic
                                    Thickness (T)
                                    Circular hollow sections
                                    Tolerances meet or exceed the requirements of EN 10219
                                    When D ≤ 323.9 mm: -5%/+10%, with a minimum of ±0.2 mm and maximum ±0.5 mm
                                    When 355.6 ≤ D ≤ 406.4 mm : ±10%, when T ≤ 5 mm / ±0.5 mm, when T > 5 mm
                                    When D > 406.4 mm : ±10%, with a maximum of ±2 mm
                                    Characteristic
                                    Straightness
                                    Circular hollow sections
                                    Tolerances meet or exceed the requirements of EN 10219
                                    0.20% of total length and 3 mm over any 1 m length
                                    Characteristic
                                    Mass per unit length
                                    Circular hollow sections
                                    Tolerances meet or exceed the requirements of EN 10219
                                    Individual tube: ±6%
                                    Characteristic
                                    Mill length
                                    Circular hollow sections
                                    Tolerances meet or exceed the requirements of EN 10219
                                    0/+50 mm, 6000 ≤ L ≤ 18000 mm (standard lengths 6000 & 12000 mm)
                                    Characteristic
                                    Exact length
                                    Circular hollow sections
                                    Tolerances meet or exceed the requirements of EN 10219
                                    Agreed at the time of enquiry and order

                                    1) All external dimensions are measured with a minimum distance from the end of the section. The distance must be a minimum of 100 mm.

                                    Tolerance Square

                                    Hide/Show specific columns Edit
                                    Select columns to display
                                      Characteristic Square hollow sections
                                      Tolerances meet or exceed the requirements of EN 10219
                                      Outside dimensions (B, H) 1) When B, H < 100="" mm="" ±1="" %="" minimum="" ±0.5="" />
                                      When 100 mm ≤ B, H ≤ 200 mm: ±0.8%
                                      When B, H > 200 mm: ±0.6%
                                      Thickness (T) -5% / +10 %, with a minimum of ±0.2 mm and maximum ±0.5 mm
                                      External corner profile When T ≤ 6 mm: 1.6 x T–2.4 x T
                                      When 6 mm < t="" ≤="" 10="" mm:="" 2.0="" x="" t-3.0="" x="" />
                                      When T > 10 mm: 2.4 x T–3.6 x T
                                      Squareness of side 90° ±1°
                                      Concavity/convexity 0.8%, with a minimum of 0.5 mm
                                      Twist 2 mm + 0.5 mm/m
                                      Straightness 0.15% of total length and 3 mm over any 1 m length
                                      Mass per unit length Individual tube: ±6%
                                      Mill length 0/+50 mm, 6000 ≤ L ≤ 18000 mm (standard lengths 6000 & 12000 mm)
                                      Exact length Agreed at the time of enquiry and order
                                      Compare parameters

                                      Select one parameter to compare

                                      Comparison

                                        Characteristic
                                        Outside dimensions (B, H) 1)
                                        Square hollow sections
                                        Tolerances meet or exceed the requirements of EN 10219
                                        When B, H < 100="" mm="" ±1="" %="" minimum="" ±0.5="" />
                                        When 100 mm ≤ B, H ≤ 200 mm: ±0.8%
                                        When B, H > 200 mm: ±0.6%
                                        Characteristic
                                        Thickness (T)
                                        Square hollow sections
                                        Tolerances meet or exceed the requirements of EN 10219
                                        -5% / +10 %, with a minimum of ±0.2 mm and maximum ±0.5 mm
                                        Characteristic
                                        External corner profile
                                        Square hollow sections
                                        Tolerances meet or exceed the requirements of EN 10219
                                        When T ≤ 6 mm: 1.6 x T–2.4 x T
                                        When 6 mm < t="" ≤="" 10="" mm:="" 2.0="" x="" t-3.0="" x="" />
                                        When T > 10 mm: 2.4 x T–3.6 x T
                                        Characteristic
                                        Squareness of side
                                        Square hollow sections
                                        Tolerances meet or exceed the requirements of EN 10219
                                        90° ±1°
                                        Characteristic
                                        Concavity/convexity
                                        Square hollow sections
                                        Tolerances meet or exceed the requirements of EN 10219
                                        0.8%, with a minimum of 0.5 mm
                                        Characteristic
                                        Twist
                                        Square hollow sections
                                        Tolerances meet or exceed the requirements of EN 10219
                                        2 mm + 0.5 mm/m
                                        Characteristic
                                        Straightness
                                        Square hollow sections
                                        Tolerances meet or exceed the requirements of EN 10219
                                        0.15% of total length and 3 mm over any 1 m length
                                        Characteristic
                                        Mass per unit length
                                        Square hollow sections
                                        Tolerances meet or exceed the requirements of EN 10219
                                        Individual tube: ±6%
                                        Characteristic
                                        Mill length
                                        Square hollow sections
                                        Tolerances meet or exceed the requirements of EN 10219
                                        0/+50 mm, 6000 ≤ L ≤ 18000 mm (standard lengths 6000 & 12000 mm)
                                        Characteristic
                                        Exact length
                                        Square hollow sections
                                        Tolerances meet or exceed the requirements of EN 10219
                                        Agreed at the time of enquiry and order

                                        1) All external dimensions are measured with a minimum distance from the end of the section. The distance must be a minimum of 100 mm.

                                        Tolerance Rectangular

                                        Hide/Show specific columns Edit
                                        Select columns to display
                                          Characteristic Rectangular hollow sections
                                          Tolerances meet or exceed the requirements of EN 10219
                                          Outside dimensions (B, H) 1) When B, H < 100="" mm="" ±1="" %="" minimum="" ±0.5="" />
                                          When 100 mm ≤ B, H ≤ 200 mm: ±0.8%
                                          When B, H > 200 mm: ±0.6%
                                          Thickness (T) -5% / +10 %, with a minimum of ±0.2 mm and maximum ±0.5 mm
                                          External corner profile When T ≤ 6 mm: 1.6 x T–2.4 x T
                                          When 6 mm < t="" ≤="" 10="" mm:="" 2.0="" x="" t-3.0="" x="" />
                                          When T > 10 mm: 2.4 x T–3.6 x T
                                          Squareness of side 90° ±1°
                                          Concavity/convexity 0.8%, with a minimum of 0.5 mm
                                          Twist 2 mm + 0.5 mm/m
                                          Straightness 0.15% of total length and 3 mm over any 1 m length
                                          Mass per unit length Individual tube: ±6%
                                          Mill length 0/+50 mm, 6000 ≤ L ≤ 18000 mm (standard lengths 6000 & 12000 mm)
                                          Exact length Agreed at the time of enquiry and order
                                          Compare parameters

                                          Select one parameter to compare

                                          Comparison

                                            Characteristic
                                            Outside dimensions (B, H) 1)
                                            Rectangular hollow sections
                                            Tolerances meet or exceed the requirements of EN 10219
                                            When B, H < 100="" mm="" ±1="" %="" minimum="" ±0.5="" />
                                            When 100 mm ≤ B, H ≤ 200 mm: ±0.8%
                                            When B, H > 200 mm: ±0.6%
                                            Characteristic
                                            Thickness (T)
                                            Rectangular hollow sections
                                            Tolerances meet or exceed the requirements of EN 10219
                                            -5% / +10 %, with a minimum of ±0.2 mm and maximum ±0.5 mm
                                            Characteristic
                                            External corner profile
                                            Rectangular hollow sections
                                            Tolerances meet or exceed the requirements of EN 10219
                                            When T ≤ 6 mm: 1.6 x T–2.4 x T
                                            When 6 mm < t="" ≤="" 10="" mm:="" 2.0="" x="" t-3.0="" x="" />
                                            When T > 10 mm: 2.4 x T–3.6 x T
                                            Characteristic
                                            Squareness of side
                                            Rectangular hollow sections
                                            Tolerances meet or exceed the requirements of EN 10219
                                            90° ±1°
                                            Characteristic
                                            Concavity/convexity
                                            Rectangular hollow sections
                                            Tolerances meet or exceed the requirements of EN 10219
                                            0.8%, with a minimum of 0.5 mm
                                            Characteristic
                                            Twist
                                            Rectangular hollow sections
                                            Tolerances meet or exceed the requirements of EN 10219
                                            2 mm + 0.5 mm/m
                                            Characteristic
                                            Straightness
                                            Rectangular hollow sections
                                            Tolerances meet or exceed the requirements of EN 10219
                                            0.15% of total length and 3 mm over any 1 m length
                                            Characteristic
                                            Mass per unit length
                                            Rectangular hollow sections
                                            Tolerances meet or exceed the requirements of EN 10219
                                            Individual tube: ±6%
                                            Characteristic
                                            Mill length
                                            Rectangular hollow sections
                                            Tolerances meet or exceed the requirements of EN 10219
                                            0/+50 mm, 6000 ≤ L ≤ 18000 mm (standard lengths 6000 & 12000 mm)
                                            Characteristic
                                            Exact length
                                            Rectangular hollow sections
                                            Tolerances meet or exceed the requirements of EN 10219
                                            Agreed at the time of enquiry and order

                                            1) All external dimensions are measured with a minimum distance from the end of the section. The distance must be a minimum of 100 mm.

                                            Contact Information

                                            www.ssab.com/contact