SSAB Virsbolt face plate
Download data sheet
Download data sheet
SSAB Virsbolt face plates are used with Virsbolt expandable rock bolts.
SSAB Virsbolt face plates are used to create a local surface support around the borehole where the Virsbolt expandable rock bolts are installed. The face plates are used to transfer the displacement of the rock mass into the rock bolt. SSAB Virsbolt face plates are used for tunneling, construction and mining.
Product | Description | Grade ASTM F432 |
Typical load capacity (kN),not guaranteed | Plate dimension(mm x mm) | Hole dimension (mm) | Thickness (mm) |
Weight(kg) |
---|---|---|---|---|---|---|---|
Dome plate adjustable 120 | Flexible plate for 120kN bolts, with an attachment hole | N/A | 50 | 150x150 | 29x39 (Oval) | 4 | Oiled: 0.67Plastic coated: 0.71 |
Dome plate adjustable 160/240 | Flexible plate for 160kN and 240kN bolts, with an attachment hole | N/A | 50 | 150x150 | 39x44 (Oval) | 4 | Oiled: 0.66Plastic coated: 0.70 |
Dome plate 120 | Plate for 120kN bolts | 2 | 100 | 152x152 | 30 (Round) | 6 | Oiled: 1.04Plastic coated: 1.08 |
Dome plate 160 240 | Plate for 160kN and 240kN bolts | 3 | 140 | 152x152 | 40 (Round) | 6 | Oiled: 1.01Plastic coated: 1.05 |
Tolerances according to SSAB specifications.
Please contact your local sales person for more information regarding tolerances.
Oiled/ plastic coated. Delivery requirements can be found in SSAB’s brochure SSAB Virsbolt, expandable rock bolt for rock reinforcement or at www.ssab.com.