Trailer Design Guideline > Economic and environmental aspects of using HSS in the trailer industry

Environmental savings

In addition to the financial benefits, a lighter vehicle will reduce environmental impact by saving primary energy resources and reducing greenhouse gas emissions.
In a life cycle assessment of a vehicle, different phases are often analyzed. When comparing an upgraded design to an original design in conventional steel, the influence of steel production and the service life is dominant. The latter often accounts for 90% of the total environmental savings for vehicles. 

When analyzing the service life of a vehicle with volume-limited cargo, the energy balance of the vehicle is considered. The basic energy consumption of road vehicles depends on several resistance factors that the vehicle has to overcome during its operation (see illustration). 

Overview of resistance factors affecting the fuel consumption of any road vehicle.

Fwi = Total resistance force
FR = Rolling resistance 
FL = Aerodynamic resistance
FSt = Gradient resistance of the road
FB = Acceleration resistance

r = Density of atmosphere
cw = Aerodynamic resistance coefficient
A = Front area
v = Speed
kr = Rolling resistance coefficient
m = Mass
a = Gradient angle
km = Acceleration resistance coefficient
a = Acceleration

Fwi = FR + FL + FSt +  FB
FR = kR • m • g • cos a
FL = r • cw • A • vx2 / 2
FSt = m • g • sin a
G = m • g
FB = km • m • ax

All resistance factors, except for aerodynamic resistance, are linearly dependent on mass. The aerodynamic resistance however, depends on the dimensions of the vehicle and the speed. As a result, energy consumption is also affected by mass, speed, acceleration, and gradient (hilly or flat). These factors are highly dependent on the driving situation and driving behavior. Assuming the same driving situation, the correlation between energy consumption and vehicle weight is linear. The energy savings corresponding to a specific weight savings is independent of the absolute weight of the vehicle.
 
Vehicles with a fast, steady speed will therefore have a high aerodynamic resistance and low acceleration resistance, and thus will have moderate specific energy savings by weight reduction. In contrast, slow vehicles with frequent stops and accelerations will have high energy savings by weight reduction. 

Contact Technical support


The information in this report is only applicable to SSAB’s products and should not be applied to any other products than original SSAB products. 


This report provides general results and recommendations for SSAB steel products. This report is subject to SSAB’s Terms of Use. It shall be the user's responsibility to verify that the information contained herein is correct and is suitable to be used for the particular purpose and application of the user. The report is intended to be used by professional users only who possess adequate expertise, qualification and knowledge for the safe and correct use of the results and recommendations in this report. This report is provided “as is”. The use of the report is at user’s own discretion and risk and that users will be solely responsible for any use of this report. SSAB disclaims any liability for the content or potential errors of this report, including but not limited to warranties and condition of merchantability or fitness for a particular purpose or suitability for individual applications. SSAB shall not be liable for any kind of direct or indirect damages and/or costs related to or arising therefrom, whether special, incidental, consequential or directly or indirectly related to the use of, or the inability to use, the report or the content, information or results included therein.