Metal coated EN10346:2015; HX220D, HX260LAD, HX300LAD, HX340LAD, HX380LAD, HX420LAD, HX500LAD
Metallbeschichtete Stähle
high-strength low alloy (HSLA) steel

Metal coated HSLA steels according to EN10346:2015

HX220D, HX260LAD, HX300LAD, HX340LAD, HX380LAD, HX420LAD, HX500LAD

Metal coated high-strength low-alloy (HSLA) steels are designed for applications that require galvanic corrosion protection and good formability in relation to high guaranteed yield strength.