How to weld > Shielding gas
Arc types for MAG welding
Each arc type is confined to certain intervals of the current and voltage that are applied during the welding operation.
A schematic diagram for the emergence of short arc and spray arc is illustrated below.
Improper settings of the current and voltage can result in the formation of a globular arc that is more unstable. It is thereby undesirable in many types of welding performances.
![](/-/media/images/technical-support/how-to-weld/shielding-gas/shielding-gas-600x470px-230616v1.png?m=20230622120209)
The short arc and spray arc appearance for different levels of current and voltage settings during MAG welding with an Ar/CO2 shielding gas mixture. Welding is typically performed with D.C.
Other welding parameters also influence the emergence of the arc types, including the chemical composition of the shielding gas, the diameter of the consumable and the stick-out length of the wire from the contact nozzle.
The information in this report is only applicable to SSAB’s products and should not be applied to any other products than original SSAB products.
This report provides general results and recommendations for SSAB steel products. This report is subject to SSAB’s Terms of Use. It shall be the user's responsibility to verify that the information contained herein is correct and is suitable to be used for the particular purpose and application of the user. The report is intended to be used by professional users only who possess adequate expertise, qualification and knowledge for the safe and correct use of the results and recommendations in this report. This report is provided “as is”. The use of the report is at user’s own discretion and risk and that users will be solely responsible for any use of this report. SSAB disclaims any liability for the content or potential errors of this report, including but not limited to warranties and condition of merchantability or fitness for a particular purpose or suitability for individual applications. SSAB shall not be liable for any kind of direct or indirect damages and/or costs related to or arising therefrom, whether special, incidental, consequential or directly or indirectly related to the use of, or the inability to use, the report or the content, information or results included therein.