How to weld > Shielding gas

Short arc MAG welding

Short arc occurs during welding with relatively low heat inputs.

This arc allows for versatile welding operations, including:

  • Out of position welding, making all types of welding positions conceivable.
  • Welding of joints with a wide range of plate thicknesses, including the complete thickness range of the Hardox® and Strenx® grades.

Some general drawbacks for short arc welding include:

  • Relatively low welding productivity.
  • The tendency toward an unstable arc. Therefore, special care should be taken in order to achieve suitable welding parameters. A good general measure is to apply a short arc length to promote a stabilized arc performance.
  • The increased risk for lack of fusion when welding in heavy plate thicknesses, due to the low heat input.

Droplet transfer at short arc welding

Short arc welding is characterized by a metal transfer from the consumable, where each droplet short- circuits the arc. The droplet transfer has a low frequency of around 50-200 Hz.

Each droplet grows to a comparatively large size during the metal transfer and then short circuits, giving a momentarily high current. The droplet leaves the wire and the arc is struck again. Short arc welding can be identified by its characteristic sparkling sound.

Illustration of short arc welding: a) Drop begins to form. b) Drop advances towards base metal. c) Drop touches weld pool, causing short circuit. d). Circuit is broken; another drop begins to form.

Category and tags

How to weldShielding gas

Contact Technical support


The information in this report is only applicable to SSAB’s products and should not be applied to any other products than original SSAB products. 


This report provides general results and recommendations for SSAB steel products. This report is subject to SSAB’s Terms of Use. It shall be the user's responsibility to verify that the information contained herein is correct and is suitable to be used for the particular purpose and application of the user. The report is intended to be used by professional users only who possess adequate expertise, qualification and knowledge for the safe and correct use of the results and recommendations in this report. This report is provided “as is”. The use of the report is at user’s own discretion and risk and that users will be solely responsible for any use of this report. SSAB disclaims any liability for the content or potential errors of this report, including but not limited to warranties and condition of merchantability or fitness for a particular purpose or suitability for individual applications. SSAB shall not be liable for any kind of direct or indirect damages and/or costs related to or arising therefrom, whether special, incidental, consequential or directly or indirectly related to the use of, or the inability to use, the report or the content, information or results included therein. 

Copyright 2026