Delivered as you like it

SSAB Boron comes in a wide range of steel grades with carbon contents from 0.22-0.42%. It is available as hot rolled plate; hot rolled coil, slit coil and sheet; cold rolled coil, slit coil and sheet; tubes and sections. Hot rolled strip products are available in black, pickled and annealed condition. Tubes and sections can be produced from hot and cold rolled base material.

CONTACT SALES

SSAB Boron – Properties guaranteed to optimize results

SSAB Boron grades

Many ways to get your steel

In order to suit your production and logistic preferences, SSAB Boron can be sourced directly from our mills or through our stocks. Please consult your local SSAB contact to design the optimal delivery solution for you.

Download SSAB Boron brochure

pdf 5,4 Mb
SSAB Boron- Optimized for you and quench hardening
Hide/Show specific columns Edit
Select columns to display
    Product Name Dimensions Standards Datasheet
    SSAB Boron 22 T: 0.70 - 80.00 mm
    W: Up to 3300 mm
    SSAB

    SSAB Boron 22

    SSAB Boron 24 T: 2.00 - 80.00 mm
    W: Up to 3300 mm
    SSAB

    SSAB Boron 24

    SSAB Boron 27 T: 2.00 - 80.00 mm
    W: Up to 3300 mm
    SSAB

    SSAB Boron 27

    SSAB Boron 27Cr T: 1.00 - 15.00 mm
    W: Up to 1800 mm
    SSAB

    SSAB Boron 27Cr

    SSAB Boron 30 T: 2.00 - 80.00 mm
    W: Up to 3300 mm
    SSAB

    SSAB Boron 30

    SSAB Boron 33 T: 2.00 - 16.00 mm
    W: Up to 1800 mm
    SSAB

    SSAB Boron 33

    SSAB Boron 33Cr T: 2.00 - 16.00 mm
    W: Up to 1800 mm
    SSAB

    SSAB Boron 33Cr

    SSAB Boron 36 T: 2.00 - 15.00 mm
    W: Up to 1800 mm
    SSAB

    SSAB Boron 36

    SSAB Boron 38 T: 1.00 - 16.00 mm
    W: Up to 1800 mm
    SSAB

    SSAB Boron 38

    SSAB Boron 42 T: 2.00 - 13.00 mm
    W: Up to 1800 mm
    SSAB

    SSAB Boron 42

    Compare parameters

    Select one parameter to compare

    Comparison

      Hide/Show specific columns Edit
      Select columns to display
        Product Name Dimensions Standards Datasheet
        SSAB Boron Tube 22 Circular: 16 - 88.9 mm
        Square: 19x19 - 70x70 mm
        Rectangular: 20x15 - 100x40 mm
        Wall Thickness: 0.9 - 3.0 mm
        EN 10305-3, EN 10305-5
        Compare parameters

        Select one parameter to compare

        Comparison

          180