180 180
Strenx 100 XF

Strenx® 100 XF

The cold-formable steel for light and heavy transportation components and solutions

Strenx® 100 XF is a thermomechanically rolled steel, made for cold forming, with a minimum yield strength of 100 ksi. It comes in coils, slit coils and cut-to-length sheets. Thickness measurements in inches can be found in the data sheet.

Strenx® 100 XF can be supplied in compliance with the requirements of ASTM A1011 or A1018 if agreed upon when you place your order.

Dimension Range

Strenx® 100 XF is available in thicknesses of 0.079 - 0.393 inches (2-10 mm), and in widths up to 63 inches (1600 mm) as coil, slit coil and as cut to length sheets in lengths up to 630 inches (16000 mm).
Strenx® 100 XF can be supplied according to ASTM A1011 or A1018 specifications if agreed up on at the time of order.

Available Standards

EN 10051

EN 10163-2 Class A, Subclass 3

Strenx 100 XF

Strenx 100 XF

USED FOR
DIMENSIONS
STANDARDS
DATA SHEET
USED FOR

Structural

DIMENSIONS

T: 2 - 10 mm

W: Up to 1600 mm

L: Up to 16000 mm

STANDARDS

EN 10051

EN 10163-2 Class A, Subclass 3

DATA SHEET

English