Highest level of durability with 50-year guarantee

GreenCoat PLX Pural BT, available in regular and matt finishes in many colors, offers the highest level of durability for standing-seam systems. It offers top Nordic quality steel, environmental benefits and durability, and come with a 50-year technical guarantee.

GreenCoat PLX Pural BT can be formed by hand with no “spring-back” and is workable at temperatures down to -15°C which many other metals do not offer. This benefit allows for cost-efficient year-round installation. It offers the highest level of durability for standing-seam systems and is highly resistant to corrosion (RC5), UV radiation (Ruv4) as well as scratches.

GreenCoat PLX Pural BT uses a bio-based coating which uses a substantial portion of Swedish rapeseed oil instead of fossil oil, which is unique on the market. SSAB holds a worldwide patent for this coating technology.

SSAB’s color coated steels comply with current REACH regulations, are fully free of chromates and are all manufactured according to EN 10169 +A1.

GreenCoat PLX – "The Roofer’s Choice"

Carl Cross, from Zinc and Copper Roofing Ltd (UK), has installed GreenCoat PLX on a roof and shares his thoughts with us. Take a look at the film."

Product details

In this section, you will find the wide range of GreenCoat® color coated products for roofing applications including technical details.
Learn more

Product details

In this section, you will find our wide product offering with our Nordic quality steels and zinc coatings recommended for different applications. Details about product dimensions are also available.

Main applications  Recommended product*  Recommended steels Recommended Zinc mass Min thickness**  Width range*** 
Roofing, tinsmith
GreenCoat PLX Pro BT PLX Z350 0.60 mm 1000-1500 mm
 GreenCoat FAP Pro BT FAP  Z350  0.60 mm 1000-1500 mm 
GreenCoat PLX Legacy PLX Z350 0.60 mm 1000-1500 mm
           
Roofing, tiles & profiles GreenCoat Pural BT S280GD, S320GD, S350GD
Z275 0.50 mm 1000-1500 mm
GreenCoat Pro BT S280GD, S320GD, S350GD
Z275 0.50 mm 1000-1500 mm
GreenCoat Mica BT S280GD, S320GD, S350GD
Z275 0.50 mm 1000-1500 mm
GreenCoat Crown BT S280GD, S320GD, S350GD
Z275 0.50 mm 1000-1300 mm
Rough Matt Polyester S280GD, S320GD, S350GD
 Z275 0.45 mm  1000-1424 mm
Polyester S280GD-S350GD, DX51D
Z275 0.42 mm 1000-1500 mm
           
Roofing, modular GreenCoat Crown BT S280GD, S320GD, S350GD Z275 0.50 mm 1000-1300 mm
           
Rain water systems GreenCoat RWS Pro FAX, PLX Z275 0.50 mm 1000-1500 mm
           
Facades GreenCoat Hiarc S280GD, S320GD, DX51D 
Z275 0.50 mm 1000-1500 mm
GreenCoat Hiarc Max S280GD, S320GD, DX51D 
Z275 0.50 mm 1000-1500 mm
GreenCoat Crown BT S280GD, S320GD
Z275 0.50 mm 1000-1300 mm
Polyester S280GD, S320GD, DX51D 
Z275 0.42 mm 1000-1500 mm
           
Indoor applications Polyester Indoor S250GD-S350GD, DX51D 
Z100 0.40 mm 1000-1424 mm
GreenCoat Foodsafe BT S250GD-S350GD, DX51D 
Z100 0.50 mm 1000-1500 mm
Laminate Foodsafe S250GD-S350GD, DX51D 
Z275 0.42 mm 1000-1400 mm
Epoxy S250GD-S350GD, DX51D 
Z100 0.40 mm 1000-1500 mm

* In addition to these we have a wide range of so called custom made products. Please contact SSAB Europe Tech support.
** Please take into account the country specific building recommendations concerning the minimum thickness. If other thicknesses are required, please contact SSAB Tech Support. Max thickness is 1,5 mm.
*** Max width depends on steel thickness. If other steel dimensions are needed, please contact SSAB Tech Support.

GreenCoat coils

GreenCoat PLX Pural BT

GreenCoat PLX Pural BT

MAIN PROPERTIES
COLOR PALETTE
DATA SHEET
MAIN PROPERTIES

Outdoor durability

Mechanical durability

Enhanced formability

Corrosion resistance

Wide color offering

Bio-based Technology (BT)

COLOR PALETTE

  • Snow White
    RR19 / SS0001

  • Quarry Grey
    RR287 / SS0244

  • Anthracite Grey
    RR2H8 / SS0087

  • Mountain Grey
    RR23 / SS0036

  • Nordic Night Black
    RR33 / SS0015

  • Chestnut Brown
    RR887 / SS0435

  • Cottage Red
    RR29 / SS0758

  • Tile Red
    RR750 / SS0760

  • Silver Fir Green
    RR5J3 / SS0975

  • Leaf Green
    RR594 / SS0874

  • Metallic Silver
    RR40 / SS0045

  • Metallic Dark Silver
    RR41 / SS0044

  • Metallic Gold
    RR42 / SS----

  • Metallic Copper
    RR979 / SS0778