180
GreenCoat Hiarc Max
GreenCoat Hiarc Max

GreenCoat Hiarc Max

It offers a PVDF-based coating specially developed for facades near a coastline

GreenCoat Hiarc offers extremely durable properties.

GreenCoat Hiarc Max is available in regular and matt finishes. Each comes in a wide range of attractive colors as well as metallic colors. GreenCoat Hiarc Max is a PVDF-based product that is extremely durable and specifically developed for facades and cassettes, but can be used also in roofing applications.

GreenCoat Hiarc Max possesses excellent weather resistance properties and tolerates forming well. It offers extremely good corrosion resistance and is well suited for buildings in the harshest environments, like those near a coastline.

Since the coating contains fluorine, the surface stays cleaner compared to other products. However, if needed the coating is also easy to clean due to hard surface. The reverse side of the sheet is painted as standard with a two-layer grey backside coating.

SSAB color coated products comply with current REACH regulations and are fully free of chromates. GreenCoat® color coated steels are all manufactured according to EN 10169 + A1.

Product details

In this section, you will find the wide range of GreenCoat® color coated products for roofing applications including technical details.
Learn more

Product details

In this section, you will find our wide product offering with our Nordic quality steels and zinc coatings recommended for different applications. Details about product dimensions are also available.

Main applications  Recommended product*  Recommended steels Recommended Zinc mass Min thickness**  Width range*** 
Roofing, tinsmith
GreenCoat PLX Pro BT PLX Z350 0.60 mm 1000-1500 mm
 GreenCoat FAP Pro BT FAP  Z350  0.60 mm 1000-1500 mm 
GreenCoat PLX Legacy PLX Z350 0.60 mm 1000-1500 mm
           
Roofing, tiles & profiles GreenCoat Pural BT S280GD, S320GD, S350GD
Z275 0.50 mm 1000-1500 mm
GreenCoat Pro BT S280GD, S320GD, S350GD
Z275 0.50 mm 1000-1500 mm
GreenCoat Mica BT S280GD, S320GD, S350GD
Z275 0.50 mm 1000-1500 mm
GreenCoat Crown BT S280GD, S320GD, S350GD
Z275 0.50 mm 1000-1300 mm
Rough Matt Polyester S280GD, S320GD, S350GD
 Z275 0.45 mm  1000-1424 mm
Polyester S280GD-S350GD, DX51D
Z275 0.42 mm 1000-1500 mm
           
Roofing, modular GreenCoat Crown BT S280GD, S320GD, S350GD Z275 0.50 mm 1000-1300 mm
           
Rain water systems GreenCoat RWS Pro FAX, PLX Z275 0.50 mm 1000-1500 mm
           
Facades GreenCoat Hiarc S280GD, S320GD, DX51D 
Z275 0.50 mm 1000-1500 mm
GreenCoat Hiarc Max S280GD, S320GD, DX51D 
Z275 0.50 mm 1000-1500 mm
GreenCoat Anti-Graffiti BT S280GD, S320GD, DX51D 
Z275 0.50 mm 1000-1500 mm
GreenCoat Crown BT S280GD, S320GD
Z275 0.50 mm 1000-1300 mm
Polyester S280GD, S320GD, DX51D 
Z275 0.42 mm 1000-1500 mm
           
Indoor applications Polyester Indoor S250GD-S350GD, DX51D 
Z100 0.40 mm 1000-1424 mm
GreenCoat Foodsafe BT S250GD-S350GD, DX51D 
Z100 0.50 mm 1000-1500 mm
Laminate Foodsafe S250GD-S350GD, DX51D 
Z275 0.42 mm 1000-1400 mm
Epoxy S250GD-S350GD, DX51D 
Z100 0.40 mm 1000-1500 mm

* In addition to these we have a wide range of so called custom made products. Please contact SSAB Europe Tech support.
** Please take into account the country specific building recommendations concerning the minimum thickness. If other thicknesses are required, please contact SSAB Tech Support. Max thickness is 1,5 mm.
*** Max width depends on steel thickness. If other steel dimensions are needed, please contact SSAB Tech Support.

GreenCoat coils

GreenCoat Hiarc Max

GreenCoat Hiarc Max

USED FOR
MAIN PROPERTIES
COATING
COLOR PALETTE
DATA SHEET
USED FOR

Facades

MAIN PROPERTIES

Outdoor durability

Dirt repellent surface

Corrosion resistance

COATING

Regular

Matt

COLOR PALETTE

  • Frost White
    RR106 / SS0009

  • Nordic White
    RR1H3 / SS0020

  • Winter White
    RR20 / SS0005

  • Fog White
    RR143 / SS----

  • Goosewing Grey
    RR2H5 / SS0461

  • Cloud Grey
    RR2B1 / SS----

  • Pebble Grey
    RR21 / SS0011

  • Stone Grey
    RR22 / SS0554

  • Mountain Grey
    RR23 / SS0036

  • Cliff Grey
    RR288 / SS0455

  • Nordic Night Black
    RR33 / SS0015

  • Walnut Brown
    RR32 / SS0387

  • Cottage Red
    RR29 / SS0758

  • Harvest Yellow
    RR24 / SS0189

  • Pine Green
    RR11 / SS0830

  • Lake Blue
    RR35 / SS0558

  • Metallic Silver
    RR40 / SS0045

  • Metallic Dark Silver
    RR41 / SS0044

  • Metallic Titanium
    RR45 / SS----

  • Metallic Gold
    RR42 / SS----

DATA SHEET