Loose sleeve splice concept of RDT piles has now extended to RDT270 and RDT320 pile sizes. Splices for both pile sizes have now been tested and are ready for use. ETA assessment will be acquired for both new splices and after that they will have CE mark. However this process takes some time and during this period there will be a statement available from Notified Body to prove the validity of the splices.

RDT splices have new type of threads which SSAB introduced in 2018. New thread profile makes tightening of threads easier and faster. Experiences of new threads have been very positive at the sites.

For availability and delivery, please contact SSAB sales.

Testing of new splices

Splices were tested for steel grades up to S550J2H and they clearly passed all the tests. Tests were done at Tampere University and followed by personnel from Eurofins Expert Services Oy, a notified body for construction products in Finland.


Figure 1. RDTs270/12.5 pile in bending test at Tampere University


Figure 2. RDTs320/12.5 piles after bending test

Since splices have same resistance as the pile pipe itself, the designer doesn’t need to consider splices in design. The structural resistance of spliced pile is the same as resistance of non-spliced piles’.

Available RD® piles with RDT loose sleeve splices

Since RDT270 and RDT320 have now also threaded RDT loose sleeve splice, the availability of different pile sizes and steel grades has widened. Available RDT pile sizes, steel grades and also the diameters of the splice sleeves are shown in Table 1 below.

Table 1. Availability of RDT splices and dimensions of RDT sleeves


More information on RD piles: RR and RD piles Design and installation manual www.ssab.com/infra

Attachments

Related articles

Jul 9Regulatory press releases
Invitation
Q2
Investors

SSAB invites you to a presentation of the Q2 2025 report at 9.30am CEST on Wednesday, July 23, 2025. The report will be published at approximately 7.30am CEST on the same date.

Jun 30Regulatory press releases
Luleå

Following the successful debt raising at the end of April 2025, SSAB has secured an additional EUR 430 million green financing to support its transformation project in Luleå, Sweden. The...

Jun 26Other press releases

SSAB has entered into an agreement with Polmotors — an innovative Tier 1 supplier — to future supplies of fossil-free steel for their structural automotive components and assemblies.