Metal coated products are made for applications that must withstand various corrosive environment, wherein they extend the service life of the end product by protecting the steel from corrosion. In addition, properly chosen metal coating makes it possible to facilitate the processing of the coated product, for instance in terms of formability, weldability and paintability.

SSAB´s offering of hot-dip metal coated products include zinc (Z), galfan (ZA) and galvannealed (ZF) coated sheet steels. The zinc coating range covers protection from Z100 up to Z600. Service life up to 80 years can be achieved with Z600 coating.