Same steel for different standards
SSAB Multisteel covers multiple steel grades and standards
Machining with all kinds of equipment is consistently stable thanks to the narrowly controlled mechanical and dimensional tolerances. The tolerance window for thickness is ¾ of the EN standard. SSAB Multisteel consistently compares favorably to standard S355 steels.
A CEV value that is lower than standard for most grades ensures excellent welding performance.
Bending properties exceed Euronorm requirements. The consistent yield strength and uniform thickness deliver predictable and repetitive spring back. Bending radius is 2 x thickness in all directions.