SSAB Boron 22

Hardenable boron steels

Boron steel is a perfect base material for a variety of products, parts and components that require resistance against abrasive wear in combination with good toughness. SSAB Boron steels are also suitable for applications calling for high strength of complex structural components. The properties of SSAB Boron 22 after heat treatment ensure longer lifetime and opportunity to weight reduction. Good forming, bending, welding and cutting properties enable the manufacture of complex components and parts. Strip products can be delivered also in annealed condition, which offers opportunity for more demanding forming.

SSAB Boron 22 has been developed to be hardened either by heat treatment after workshop processing or by a direct hot forming and quenching process to obtain final properties.

SSAB Boron 22 is delivered in hot rolled (as-rolled) condition as heavy plates, coils, slit coils and cut-to-length sheets and in cold-rolled condition as coils, slit coils and cut to length.

Dimension Range

SSAB Boron 22 is available in thickness range 0.70-80.00 mm and widths up to 1800 mm as coils, slit coils and CTL and 3300 mm as plate. Lengths up to 16 meters as cut to length.

Available Standards

EN 10131

EN 10051

EN 10029

EN 10163-2 Class A, Subclass 3

SSAB Boron 22

SSAB Boron 22

USED FOR
DIMENSIONS
STANDARDS
DATA SHEET
USED FOR

Boron (hardening)

Wear Resistant

DIMENSIONS

T: 0.7 - 80 mm

W: Up to 3300 mm

L: Up to 16000 mm

STANDARDS

EN 10131

EN 10051

EN 10029

EN 10163-2 Class A, Subclass 3

DATA SHEET