For high quality rainwater systems.
GreenCoat RWS Pural color coated steel is available in regular finish and offers a wide range of colors inspired by Nordic nature.
GreenCoat RWS Pural offers the highest level of durability for rainwater systems using a double-sided coating (same coating is applied on both sides of the sheet).
GreenCoat RWS Pural color coated steel provides excellent corrosion resistance (RC5), gloss retention and color fastness (Ruv5). GreenCoat RWS Pural possesses excellent forming properties enabling very demanding folding even down to -15°C, allowing for year round installation at lower costs.
Excellent weather resistance together with regular maintenance and the cleaning of rainwater systems can maximize the service life of the product.
GreenCoat RWS Pural complies with current REACH regulations and is fully chromate-free.
SSAB’s color coated steels are all manufactured according to EN 10169.