Other press releases

Modernization of pickling line entry section completed at SSAB Hämeenlinna

Automotive, Investment, Strategy
December 13, 2018 9:00 CET
SSAB’s investment project to modernize the entry section of the pickling line at the Hämeenlinna Works has now been completed. The investment supports SSAB’s growth strategy in the automotive industry and enables a higher production volume of more advanced coated strip products.

Metal-coated strip products are sold directly to customers in the automotive and construction industries, and they are also further processed into color-coated products on our color-coating lines.

“Modernization makes the line better suited to the manufacture of high-strength steel grades for the automotive industry for example,” said Olavi Huhtala, Head of SSAB Europe.

SSAB’s investment of some SEK 370 million in modernizing the entry section of the pickling line at the Hämeenlinna Works included the mechanical, electrical and automation equipment as well as new electrical and automation premises, an entry section control room and scale dust removal devices. 

“The new laser welding machine enables demanding steel grades used by the automotive industry to be welded more smoothly. The scalebreaker improves pickling line performance thereby making the entire process more efficient,” said Olavi Huhtala.

All products made in Hämeenlinna pass along the pickling line, where a hydrochloric acid solution removes scale and iron oxide from the steel strip surface before cold-rolling and metal-coating. SSAB successfully ran production at a normal pace during the two years of construction work, apart some short outages.

For further information, please contact:
Olavi Huhtala, Head of SSAB Europe, and tel. + 358 20 592 9157

Attachments

Modernization of pickling line entry section completed at SSAB Hämeenlinna

Related articles

Other press releasesSSAB invests in its Nordic operations
Automotive, Investment, Strategy, Production
Other newsExcellent teamwork and communication ensured the successful launch of Docol 1500M-EG
Automotive, Docol, Strategy
Other newsAutomotive growth – capitalizing on lightweighting and safety trends
Automotive, Strategy