Slurry pipelines, stone quarry tubes and pipes in Hardox® wear plate
If you want to increase the lifetime of slurry pipelines, tubes used in stone quarries and other pipes subject to wear and abrasion, you’ve got many good reasons to try out Hardox® tubes.
Field tests have proved that Hardox® Tube 400 and Hardox® Tube 500, with a hardness grade of 400 HB and 500 HB, last 2.5 and 4 times longer, respectively, than mild steel when pumping wet concrete. Hardox® tubes were also successfully introduced in pneumatic powder conveying systems for clinker and glass. They also deliver superior wear resistance in other mining machinery and equipment.
Hard-working screening buckets rely on Hardox® tubes
Remu Oy has been using Hardox® steel for a long time and knows that this wear-resistant material is second to none. The proof is in the high productivity and long-lasting performance of its products.
Hardox® wear plate: The unrivaled choice for extreme wear challenges
Survival of the fittest. Built for extended service life and high productivity in the most extreme conditions, Hardox® wear plate is the leading abrasion-resistant steel – hard through and through, from surface to core. Why settle for anything else?