How to weld > Magnetic arc blow

Residual magnetism in steels

Ferromagnetic steels, including the Hardox® and Strenx® grades, can contain varying levels of residual magnetism.

The  magnetic flux density gradually lowers as the distance from the electrode increases. When it is high enough, this magnetism can interfere with the magnetic field from the welding torch and cause magnetic arc blow. Common sources that enhance the magnetism of the steel include:

  • Magnets used in jacking equipment
  • Storage in a place with high levels of magnetic flux densities.

 

Low levels of magnetism in the joint will not influence the stability of the arc. Arc blow disturbances can occur when the magnetic flux density is approximately 40 Gauss or above.

The Hardox® and the Strenx® grades are high strength steels with favorable resistance to residual magnetism. However, there are instances when they can obtain magnetic flux densities of 40 Gauss or more. The sensitivity towards magnetic arc blow, caused by residual magnetism in the steel, is generally more emphasized with:

  • Hardox® grades of higher hardness
  • Higher strength Strenx® grades.

The objective in the following context is to further describe the nature of magnetic arc blow. Suitable remedies are then provided on how to counteract this effect.

Contact Technical support


The information in this report is only applicable to SSAB’s products and should not be applied to any other products than original SSAB products. 


This report provides general results and recommendations for SSAB steel products. This report is subject to SSAB’s Terms of Use. It shall be the user's responsibility to verify that the information contained herein is correct and is suitable to be used for the particular purpose and application of the user. The report is intended to be used by professional users only who possess adequate expertise, qualification and knowledge for the safe and correct use of the results and recommendations in this report. This report is provided “as is”. The use of the report is at user’s own discretion and risk and that users will be solely responsible for any use of this report. SSAB disclaims any liability for the content or potential errors of this report, including but not limited to warranties and condition of merchantability or fitness for a particular purpose or suitability for individual applications. SSAB shall not be liable for any kind of direct or indirect damages and/or costs related to or arising therefrom, whether special, incidental, consequential or directly or indirectly related to the use of, or the inability to use, the report or the content, information or results included therein.