How to weld > Shielding gas

Argon

Argon also enhances the formation of the spray arc transfer.

However, a 100% argon shielding gas would lead to an unstable arc so the shielding gases need to include another gas component that has the ability to stabilize the arc.

Argon promotes a narrow and intense arc that produces a deep penetration profile in the center of the weld metal, often called the argon finger, see illustration below. It lowers the heat transfer capacity in the melt during welding; contributing to a narrower penetration profile for each weld pass.

The penetration profile promoted by a shielding gas with high argon content.

The negative effects from a relatively small and narrow penetration profile include an increased risk for lack of fusion in the joint. In addition, it result in a somewhat higher susceptibility towards porosity in the weld metal.

Category and tags

How to weldShielding gas

Contact Technical support


The information in this report is only applicable to SSAB’s products and should not be applied to any other products than original SSAB products. 


This report provides general results and recommendations for SSAB steel products. This report is subject to SSAB’s Terms of Use. It shall be the user's responsibility to verify that the information contained herein is correct and is suitable to be used for the particular purpose and application of the user. The report is intended to be used by professional users only who possess adequate expertise, qualification and knowledge for the safe and correct use of the results and recommendations in this report. This report is provided “as is”. The use of the report is at user’s own discretion and risk and that users will be solely responsible for any use of this report. SSAB disclaims any liability for the content or potential errors of this report, including but not limited to warranties and condition of merchantability or fitness for a particular purpose or suitability for individual applications. SSAB shall not be liable for any kind of direct or indirect damages and/or costs related to or arising therefrom, whether special, incidental, consequential or directly or indirectly related to the use of, or the inability to use, the report or the content, information or results included therein.