Electrogalvanized AHSS steels

Electrogalvanizing AHSS steel involves electrolytically depositing a layer of zinc by running the steel through a conducting zinc salt bath with inert anodes and the steel strip as the cathode.

Electrogalvanizing provides a uniform coating and high surface quality. EG coats are much thinner than other galvanizing processes, making them appropriate when the thinnest possible coating is needed for corrosion protection.

SSAB offers various EG-coated AHSS steels; particularly noteworthy are our electrogalvanized martensitic grades. Electrogalvanized coatings are designated as EG by the VDA standards and ZE by the EN nomination.

Formability of electrogalvanized AHSS

Electrogalvanized coatings can be suitable for highly formed (e.g., deeply drawn) automotive parts. Lubrication prior to forming may be needed for some extreme applications.

Weldability of electrogalvanized AHSS

Electrogalvanizing provides excellent resistance spot welding properties.

Adhesive and mechanical joining of electrogalvanized AHSS

Electrogalvanized AHSS steel can be joined using a variety of adhesives. EG-coated parts are generally considered easier to bond than traditional zinc-coated (GI) parts. Mechanical joining of electrogalvanized parts can be done using bolts, rivet tabs, or non-tabs.

Electrogalvanized: EG/ZE electrolytic zinc coatings

Available on select:

  • Docol Martensitic
  • Docol Complex Phase
  • Docol Dual Phase

Select from the full range of Docol corrosion-resistant AHSS

Download the list of our 50+ currently available coated automotive steels, plus the 20 new offerings available for your trial testing

pdf 2,64 Mb
Docol® Product program for the automotive industry

Is electrogalvanized AHSS right for your vehicle?

Our Knowledge Service Center experts can help you select the right corrosion protection for your BIW component. Contact your local Docol Representative.

Need to review the full offering of Docol automotive AHSS steels? Then please visit our steels overview page.

icon learn
180