    General Product Description

    Docol 1200CP complex phase steel is developed for increased safety in cars. Its ultra-high strength combined with an improved formability allows for weight reduction in BIW applications. This steel undergoes special heat treatment in a continuous annealing or galvanizing line, producing a complex phase structure.

    Dimension Range

    Cold rolled / UC, EG: thickness 0.50-2.10 mm, width up to 1527 mm.

    Cold rolled / GI: thickness 1.00-1.70 mm, width up to 1350 mm.

    Slit strip are available upon request.

    Grade and coating specific restrictions on available dimensions may occur.

    Mechanical Properties

    Hide/Show specific columns Edit
    Select columns to display
      Standard Coating Test direction
      Yield strength Rp0.2
      (MPa)
      Tensile strength Rm
      (MPa)
      Elongation A80
      (min %)
      BH2
      (min MPa)
      Docol CR​900Y​1180T-​CP VDA 239-100 UC, EG, GI* L 900 - 1100 1180 - 1350 5 30
      Compare parameters

      Select one parameter to compare

      Comparison

        The testing of mechanical properties of electrogalvanized products is conducted without coating.

        * Available upon request

        Chemical Composition (ladle analysis)

        Hide/Show specific columns Edit
        Select columns to display
          Coating C
          (max %)
          Si
          (max %)
          Mn
          (max %)
          P
          (max %)
          S
          (max %)
          Al
          (%)
          Nb+Ti
          (max %)
          Cr+Mo
          (max %)
          B
          (max %)
          Cu
          (max %)
          Docol CR​900Y​1180T-​CP UC, EG, GI* 0.23 1.00 2.90 0.050 0.010 0.015 - 1.00 0.15 1.00 0.005 0.20
          Compare parameters

          Select one parameter to compare

          Comparison

            * Available upon request.

            Tolerances

            Cold rolled (UC, EG): Tolerances in accordance to EN 10131.

            Hot-dip galvanized (GI): Tolerances in accordance to EN 10143.

            Customized dimensional and shape tolerances are available upon request.

            Coatings

            The metal coating options for Docol products include:

            Hot-dip zinc coating (GI) consists almost entirely of zinc (>99%). It is lead free, resulting in a small zinc spangle size. The coating provides good corrosion protection.

            Electrogalvanized coating (EG) is applied continuously by electro deposition. The coating consists of zinc (>99%). Electrogalvanized steel is characterized by its excellent surface quality and uniform coating thickness.

            Grade specific availability of metal coatings for Docol products is given in the Mechanical properties table (Coating).

            Hide/Show specific columns Edit
            Select columns to display
              Coating type Coating class Standard Closest in EN standard, informative 1) Coating mass per side, single spot test (g/m2) Thickness per side informative (µm)
              GI 40/40 VDA 239-100 Z100 40 - 60 5.6 - 8.5
              GI 50/50 VDA 239-100 50 - 70 7.0 - 9.9
              GI 60/60 VDA 239-100 Z140 60 - 90 8.5 - 12.7
              GI 70/70 VDA 239-100 70 - 100 9.9 - 14.1
              GI 85/85 VDA 239-100 85 - 115 12.0 - 16.2
              GI 115/115 VDA 239-100 Z275 115 - 155 16.2 - 21.8
              EG 12/12 VDA 239-100 ZE25/25 12 - 32 1.7 - 4.5
              EG 18/18 VDA 239-100 18 - 38 2.5 - 5.4
              EG 29/29 VDA 239-100 ZE50/50 29 - 49 4.1 - 6.9
              EG 47/47 VDA 239-100 ZE75/75 47 - 61 6.6 - 8.6
              EG 50/50 VDA 239-100 50 - 70 7.0 - 9.9
              EG 53/53 VDA 239-100 53 - 73 7.5 - 10.3
              EG 60/60 VDA 239-100 60 - 80 8.5 - 11.3
              EG 65/65 VDA 239-100 ZE100/100 65 - 85 9.2 - 12.0
              EG 70/70 VDA 239-100 70 - 90 9.9 - 12.7
              Compare parameters

              Select one parameter to compare

              Comparison

                Docol metal coated products are available with surface quality for unexposed applications.

                In addition to these coating masses, OEM specific coatings and single sided EG coatings are available upon request.

                1) For GI and GA the closest informative value refers to EN 10346. For EG to EN 10152.

                Surface Treatments

                Uncoated (UC): available as oiled.

                Hot-dip galvanized (GI): available as oiled and/or chemically passivated.

                Electrogalvanized (EG): available as oiled and/or chemically passivated or phosphated.

                All surface treatments are in accordance with RoHS directive (2011/65/EU) and do not contain Chromium VI (Cr6+). Surface treatments provide only temporary surface protection during transportation and storage. In order to avoid corrosion damages, care must be taken to keep the products dry during transportation and storage. If they become wet, they must be separated and situated so that they are dried quickly.

                Fabrication and Other Recommendations

                For information concerning fabrication, see SSAB´s brochures on www.ssab.com or consult Tech Support.

                Appropriate health and safety precautions must be taken when bending, welding, cutting, grinding or otherwise working on the products.