SSAB Domex Tube 235 JRH

SSAB Domex® Tube 235 JRH

Hollow section for general applications

SSAB Domex® Tube 235 J2H is cold formed advanced structural hollow section

It meets or exceeds the requirements of standard EN 10219 and is available in circular, rectangular, square and special shapes. It is typically used in advanced engineering and construction where lower costs and safety are important. It has very clean chemistry and uniform quality. The impact ductility is tested at -40°C and it is suitable for high quality hot-dip galvanizing. Also welding in corner areas is always permitted.

SSAB Domex® Tube 235 J2H is manufactured by cold forming and high frequency welding from clean, high quality environmentally friendly steel by modern and efficient tube lines.

Mitta-alue

SSAB Domex Tube 235 J2H -rakenneputkia on saatavilla pyöreinä, neliönmuotoisina ja suorakulmaisina. 

Pyöreä 42,4–323,9 mm 
Neliönmuotoinen 40 x 40 – 300 x 300 mm 
Suorakulmainen 50 x 30 – 400 x 200 mm 
Seinämän paksuus 2,0–12,50 mm
Pituus 6 000 / 12 000 mm

Saatavilla olevat standardit

EN 10219-1

EN 10219-2

Valitse muoto, jotta voit näyttää ominaisuudet