SSAB Multisteel PE

Datenblatt herunterladen

Sprache wählen

Get datasheet by email
Schließen

Get datasheet by email

    Allgemeine Produktbeschreibung

    Normalized pressure vessel steel heavy plate.

    SSAB Multisteel PE is hot rolled structural steel for general pressure equipment steel constructions. PE = Pressure European (meets the European standard).

    Exceeding the requirements of several standard steel grades, SSAB Multisteel PE is a versatile pressure vessel steel for fabricated pressure equipment made of weldable fine grain steels. Formability and highly consistent quality guarantee fast, uninterrupted production, generating clear savings in the costs of material management.

    SSAB Multisteel PE exceeds several steel standards and is available as four steel grades: P355N, P355NH, P355NL1 and P355NL2 according to EN 10028-3.

    SSAB Multisteel PE covers steel grades in four different qualities:

    1) Room temperature quality (P355N)

    2) Elevated temperature quality (P355NH)

    3) Low temperature quality (P355NL1)

    4) Special low temperature quality (P355NL2)

    5) SSAB Multisteel PE (all together)

    PED certificate:

    Pressure vessel steel grades recognized by standard EN 10028 are mainly delivered with the inspection certificate 3.1. Directive 2014/68/EU (PED) requires the manufacturer’s quality assurance system to be approved by an external accredited authority (Notified Body).

    SSAB Europe Oy Raahe Works holds the PED – approval from DNV.

    SSAB Raahe Works is authorized to use PED certificate for pressure equipment steels according to EN 10028-3 based on EN 10028-1.

    Abmessungsbereich

    SSAB Multisteel PE is available in thickness of 5.00 – 150.00 mm.

    Mechanische Eigenschaften

    Bestimmte Spalten ein-/ausblenden Bearbeiten
    Spalten zur Anzeige auswählen
      Dicke
      (mmin)
      Streckgrenze
      (min MPa)
      Zugfestigkeit
      (MPa)
      Bruchdehnung A5
      (min %)
      6.00 - 16.000.236 - 0.6299 355 490 - 630 22
      16.01 - 40.000.6303 - 1.575 345 490 - 630 22
      40.01 - 60.001.575 - 2.362 335 490 - 630 22
      60.01 - 100.002.363 - 3.9370 315 470 - 610 21
      100.01 - 150.003.9374 - 5.9055 305 460 - 600 21
      Parameter vergleichen

      Wählen Sie einen zu vergleichenden Parameter aus

      Vergleich

        The mechanical properties are tested transverse to the direction of rolling.

        Hot tensile test is performed at +300°C in compliance with EN 10028-3 and EN 10028-1.

        Kerbschlagarbeit

        Bestimmte Spalten ein-/ausblenden Bearbeiten
        Spalten zur Anzeige auswählen
          Mind. Aufprallenergie für Längsprüfung,
          Charpy V 10x10- Kerbschlagversuch
          SSAB Multisteel PE 27 J / -50 °C
          EN 10028-3 P355N, P355NH 30 J / -20 °C
          EN 10028-3 P355NL1 27 J / -40 °C
          EN 10028-3 P355NL2 27 J / -50 °C
          Parameter vergleichen

          Wählen Sie einen zu vergleichenden Parameter aus

          Vergleich

            SSAB Multisteel PE
            Mind. Aufprallenergie für Längsprüfung,
            Charpy V 10x10- Kerbschlagversuch
            27 J / -50 °C
            EN 10028-3 P355N, P355NH
            Mind. Aufprallenergie für Längsprüfung,
            Charpy V 10x10- Kerbschlagversuch
            30 J / -20 °C
            EN 10028-3 P355NL1
            Mind. Aufprallenergie für Längsprüfung,
            Charpy V 10x10- Kerbschlagversuch
            27 J / -40 °C
            EN 10028-3 P355NL2
            Mind. Aufprallenergie für Längsprüfung,
            Charpy V 10x10- Kerbschlagversuch
            27 J / -50 °C

            The impact test is made transverse to the rolling direction in compliance with EN 10028-3 and EN 10028-1.

            Chemische Zusammensetzung (Schmelzenanalyse)

            Bestimmte Spalten ein-/ausblenden Bearbeiten
            Spalten zur Anzeige auswählen
              C
              (max %)
              Si
              (max %)
              Mn
              (max %)
              P
              (max %)
              S
              (max %)
              Nb
              (max %)
              0.18 0.50 1.70 0.020 0.005 0.05
              Parameter vergleichen

              Wählen Sie einen zu vergleichenden Parameter aus

              Vergleich

                Kohlenstoffäquivalent CEV

                Bestimmte Spalten ein-/ausblenden Bearbeiten
                Spalten zur Anzeige auswählen
                  Dicke (mmin) 5.00 - 50.000.197 - 1.969 50.01 - 150.001.969 - 5.9055
                  CEV
                  (max %)
                  0.43 0.45
                  Parameter vergleichen

                  Wählen Sie einen zu vergleichenden Parameter aus

                  Vergleich

                    Toleranzen

                    Thickness ¾ from EN 10029 Class B.

                    Width and length according to EN 10029.

                    Flatness tolerance 6 mm/m.

                    Surface according to EN 10163-2 Class B subclass 3.

                    Lieferzustand

                    Normalized.

                    Beschichtungen

                    Shot blasted & primed surface is available upon request.

                    Certificates

                    SSAB Multisteel PE provides two different certificates:

                    EN 10204-3.1 to SSAB Multisteel PE.

                    EN 10204-3.1/PED2014/68/EU to P355NL1/NL2/NH/N EN 10028-3.

                    Verarbeitung und andere Empfehlungen

                    Welding:

                    Weldability is excellent with all welding processes. Increased working temperature requirements are less than those of the corresponding strength grades of standard steels. This means easier welding and cost savings under both workshop and site welding conditions.

                    Needed working temperatures for thick plates please consult SSAB Tech Support.

                    Forming:

                    SSAB Multisteel offers better formability properties than standard steels. Successful forming requires that the manufacturer uses good workshop techniques. Worn tools, poor lubrication, scratches on the surface of the steel as well as edge burrs will all reduce forming quality.

                    Guaranteed minimum bending radius for all directions is 2 x t up to 30 mm thick plate where t = plate thickness.

                    Heat treatment:

                    Recommendations for stress relieving and normalizing.

                    Stress relieving 550 – 600°C (target 580°C)

                    2 minutes/millimeter of thickness, however, 30 minutes minimum. Slow cooling in the furnace.

                    Normalizing 900 – 940°C (target 920°C)

                    1 minute/millimeter of thickness, however, 20 minutes minimum. Cooling in free air.

                    Informationen bezüglich Schweißbarkeit und Verarbeitung finden Sie in den SSAB Broschüren auf www.ssab.com oder kontaktieren Sie die Technische Kundenbetreuung

                    Entsprechende Sicherheits- und Gesundheitsvorkehrungen müssen beim Schweißen, Schneiden, Schleifen oder anderen Arbeiten mit dem Produkt getroffen werden.