Produktname | Abmessungen | Normen | Datenblatt |
|---|---|---|---|
| SSAB Laser® 250C | T: 2.0 - 30.0 mm W: 1000 - 3300 mm L: 1000 - 16000 mmT: 0.079 - 1.18 in W: 39.37 - 129.9 in L: 39.37 - 629.92 in | EN 10025-2 | |
| SSAB Laser® 275C | T: 2.0 - 30.0 mm W: 1000 - 3300 mm L: 1000 - 16000 mmT: 0.079 - 1.18 in W: 39.37 - 129.9 in L: 39.37 - 629.92 in | EN 10025-2 | |
| SSAB Laser® 355C | T: 3.0 - 30.0 mm W: 1000 - 3300 mm L: 1000 - 16000 mmT: 0.12 - 1.18 in W: 39.37 - 129.9 in L: 39.37 - 629.92 in | EN 10025-2 | |
| SSAB Laser® 355ML Plus | T: 8.0 - 30.0 mm W: 1000 - 3300 mm L: 2000 - 15000 mmT: 0.31 - 1.18 in W: 39.37 - 129.9 in L: 78.74 - 590.55 in | EN 10025-4 | |
| SSAB Laser® 420ML Plus | T: 10.0 - 25.0 mm W: 1000 - 3300 mm L: 2000 - 15000 mmT: 0.394 - 0.984 in W: 39.37 - 129.9 in L: 78.74 - 590.55 in | EN 10025-4 | |
| SSAB Laser® 460ML Plus | T: 10.0 - 25.0 mm W: 1000 - 3300 mm L: 2000 - 15000 mmT: 0.394 - 0.984 in W: 39.37 - 129.9 in L: 78.74 - 590.55 in | EN 10025-4 |
SSAB Laser® 250C
SSAB Laser® 275C
SSAB Laser® 355C
SSAB Laser® 355ML Plus
SSAB Laser® 420ML Plus
SSAB Laser® 460ML Plus