SSAB Multisteel SNL

Datenblatt herunterladen

Sprache wählen

    Allgemeine Produktbeschreibung

    Normalized structural steel heavy plate.

    SSAB Multisteel SNL is hot rolled structural steel for general steel constructions. SNL = Structural Normalized Low Temperature.

    Exceeding the requirements of several standard steel grades, SSAB Multisteel SNL is a versatile structural steel for fabricated products and steel frame structures. Formability and highly consistent quality guarantee fast, uninterrupted production, generating clear savings in the costs of material management.

    SSAB Multisteel SNL exceeds several steel standards and is available as six standard steel grades: S355N and S355NL according to EN 10025-3 and S355K2+N, S355J2+N, S355J0+N and S355JR+N according to EN 10025-2.

    CE marking:

    SSAB Raahe Works is authorized to use the CE marking for structural steels according to EN 10025-2 and EN 10025-3 based on EN 10025-1.

    The CE marking is marked on an extra page of inspection certification 3.1.

    Abmessungsbereich

    SSAB Multisteel SNL is available in thickness of 5.00 - 150.00 mm.

    Mechanische Eigenschaften

    Bestimmte Spalten ein-/ausblenden Bearbeiten
    Spalten zur Anzeige auswählen
      Dicke
      (mm)
      Streckgrenze
      (min MPa)
      Zugfestigkeit
      (MPa)
      Bruchdehnung A5
      (min %)
      5.00 - 16.00 355 470 - 630 22
      16.01 - 40.00 345 470 - 630 22
      40.01 - 63.00 335 470 - 630 22
      63.01 - 80.00 325 470 - 630 21
      80.01 - 100.00 315 470 - 630 21
      100.01 - 150.00 295 450 - 600 21
      Parameter vergleichen

      Wählen Sie einen zu vergleichenden Parameter aus

      Vergleich

        The mechanical properties are tested transverse to the direction of rolling.

        Kerbschlagarbeit

        Bestimmte Spalten ein-/ausblenden Bearbeiten
        Spalten zur Anzeige auswählen
          Mind. Aufprallenergie für Längsprüfung,
          Charpy V - Kerbschlagversuch
          SSAB Multisteel SNL 27 J / -50 °C
          EN 10025-3 S355NL 27 J / -50 °C
          EN 10025-3 S355N 40 J / -20 °C
          EN 10025-2 S355K2+N 40 J / -20 °C
          EN 10025-2 S355J2+N 27 J / -20 °C
          EN 10025-2 S355J0+N 27 J / 0 °C
          EN 10025-2 S355JR+N J / °C
          Parameter vergleichen

          Wählen Sie einen zu vergleichenden Parameter aus

          Vergleich

            The impact test is made longitudinal to the rolling direction in compliance with EN 10025-1 and EN 10025-2.

            Chemische Zusammensetzung (Schmelzenanalyse)

            Bestimmte Spalten ein-/ausblenden Bearbeiten
            Spalten zur Anzeige auswählen
              C
              (max %)
              Si
              (max %)
              Mn
              (max %)
              P
              (max %)
              S
              (max %)
              Nb
              (max %)
              0.18 0.50 1.60 0.020 0.010 0.05
              Parameter vergleichen

              Wählen Sie einen zu vergleichenden Parameter aus

              Vergleich

                Kohlenstoffäquivalent CEV

                Bestimmte Spalten ein-/ausblenden Bearbeiten
                Spalten zur Anzeige auswählen
                  Dicke (mm) 5.00 - 63.00 63.01 - 150.00
                  CEV
                  (max )
                  0.43 0.45
                  Parameter vergleichen

                  Wählen Sie einen zu vergleichenden Parameter aus

                  Vergleich

                    Toleranzen

                    Thickness ¾ from EN 10029 Class A.

                    Width and length according to EN 10029.

                    Flatness tolerance 4 mm/m.

                    Surface according to EN 10163-2 Class A subclass 1.

                    Lieferzustand

                    Normalized.

                    Beschichtungen

                    Shot blasted & primed surface is available upon request.

                    Certificates

                    SSAB Multisteel SNL provides three different certificates:

                    EN 10204-3.1 to SSAB Multisteel SNL.

                    EN 10204-3.1 +CE to S355NL/N EN 10025-3.

                    EN 10204-3.1 +CE to S355K2/J2/J0/JR+N EN 10025-2.

                    Verarbeitung und andere Empfehlungen

                    Welding:

                    Weldability is excellent with all welding processes. Increased working temperature requirements are less than those of the corresponding strength grades of standard steels. This means easier welding and cost savings under both workshop and site welding conditions.

                    Needed working temperatures for thick plates please consult SSAB Tech Support.

                    Forming:

                    SSAB Multisteel offers better formability properties than standard steels. Successful forming requires that the manufacturer uses good workshop techniques. Worn tools, poor lubrication, scratches on the surface of the steel as well as edge burrs will all reduce forming quality.

                    Guaranteed minimum bending radius for all directions is 1.5 x t up to 30 mm thick plate where t = plate thickness.

                    Heat treatment:

                    Recommendations for stress relieving and normalizing

                    Stress relieving 550 – 600°C (target 580°C)

                    2 minutes/millimeter of thickness, however, 30 minutes minimum. Slow cooling in the furnace.

                    Normalizing 900 – 940°C (target 920°C)

                    1 minute/millimeter of thickness, however, 20 minutes minimum. Cooling in free air.

                    Informationen bezüglich Schweißbarkeit und Verarbeitung finden Sie in den SSAB Broschüren auf www.ssab.com oder kontaktieren Sie die Technische Kundenbetreuung

                    Entsprechende Sicherheits- und Gesundheitsvorkehrungen müssen beim Schweißen, Schneiden, Schleifen oder anderen Arbeiten mit dem Produkt getroffen werden.

                    Kontakt Information

                    www.ssab.com/contact