Strenx Tube 960MH
Advanced high-strength structural hollow sections

Strenx® Tube 960MH

Advanced high-strength structural hollow sections

Strenx® Tube 960MH is an HF-welded cold-formed structural hollow section made of hot-rolled high-strength steel with a minimum yield strength of 960 MPa.

Its high strength combined with naturally stiff form of welded hollow section enables construction of stronger and lighter structures. Strenx® Tube 960MH meets or exceeds the requirements of prEN 10219-3 (2020). Typical applications include load-bearing structures in the lifting, handling and transportation segments.

Strenx® Tube 960MH is available in circular, square and rectangular shapes. Other shapes and sizes are available upon request.

The maximum length of the tubes is 12-18 meters, depending on the size. Longer or cut-to-length tubes are available upon request.

It is not recommended to hot dip galvanize Strenx® Tube 960MH hollow sections.

Abmessungsbereich

Strenx® Tube 960MH ist in runden, quadratischen und rechteckigen Formen lieferbar. 

   
Rund 139.7- 244.5 mm 
Quadratisch   100 x 100 - 200 x 200 mm 
Rechteckig 120 x 80 - 250 x 150 mm 
Wanddicke 4.0 - 6.0 mm
Rohrlänge 6.000 - 12.000/18.000 mm

Andere Formen und Abmessungen sind auf Anfrage erhältlich.

Verfügbare Normen

EN 10219-2