    Allgemeine Produktbeschreibung

    Normalized or normalized rolled structural steel heavy plate.

    SSAB Multisteel SN is hot rolled structural steel for general steel constructions. SN = Structural Normalized.

    Exceeding the requirements of several standard steel grades, SSAB Multisteel SN is a versatile structural steel for fabricated products and steel frame structures. Formability and highly consistent quality guarantee fast, uninterrupted production, generating clear savings in the costs of material management.

    SSAB Multisteel SN exceeds several steel standards and is available as four standard steel grades: S355K2+N, S355J2+N, S355J0+N and S355JR+N according to EN 10025-2.

    CE marking:

    SSAB Raahe Works is authorized to use the CE marking for structural steels according to EN 10025-2 based on EN 10025-1.

    The CE marking is marked on an extra page of inspection certification 3.1.

    Abmessungsbereich

    SSAB Multisteel SN is available in thickness of 5.00 - 150.00 mm.

    Mechanische Eigenschaften

    Bestimmte Spalten ein-/ausblenden Bearbeiten
    Spalten zur Anzeige auswählen
      Dicke
      (mm)
      Streckgrenze
      (min MPa)
      Zugfestigkeit
      (MPa)
      Bruchdehnung A5
      (min %)
      5.00 - 16.00 355 470 - 630 21
      16.01 - 40.00 345 470 - 630 21
      40.01 - 63.00 335 470 - 630 20
      63.01 - 80.00 325 470 - 630 19
      80.01 - 100.00 315 470 - 630 19
      100.01 - 150.00 295 450 - 600 19
      Parameter vergleichen

      Wählen Sie einen zu vergleichenden Parameter aus

      Vergleich

        The mechanical properties are tested transverse to the direction of rolling.

        Kerbschlagarbeit

        Bestimmte Spalten ein-/ausblenden Bearbeiten
        Spalten zur Anzeige auswählen
          Mind. Aufprallenergie für Längsprüfung,
          Charpy V - Kerbschlagversuch
          SSAB Multisteel SN 40 J / -20 °C
          EN 10025-2 S355K2+N 40 J / -20 °C
          EN 10025-2 S355J2+N 27 J / -20 °C
          EN 10025-2 S355J0+N 27 J / 0 °C
          EN 10025-2 S355JR+N J / °C
          Parameter vergleichen

          Wählen Sie einen zu vergleichenden Parameter aus

          Vergleich

            SSAB Multisteel SN
            Mind. Aufprallenergie für Längsprüfung,
            Charpy V - Kerbschlagversuch
            40 J / -20 °C
            EN 10025-2 S355K2+N
            Mind. Aufprallenergie für Längsprüfung,
            Charpy V - Kerbschlagversuch
            40 J / -20 °C
            EN 10025-2 S355J2+N
            Mind. Aufprallenergie für Längsprüfung,
            Charpy V - Kerbschlagversuch
            27 J / -20 °C
            EN 10025-2 S355J0+N
            Mind. Aufprallenergie für Längsprüfung,
            Charpy V - Kerbschlagversuch
            27 J / 0 °C
            EN 10025-2 S355JR+N
            Mind. Aufprallenergie für Längsprüfung,
            Charpy V - Kerbschlagversuch
            J / °C

            The impact test is made longitudinal to the rolling direction in compliance with EN 10025-1 and EN 10025-2.

            Chemische Zusammensetzung (Schmelzenanalyse)

            Bestimmte Spalten ein-/ausblenden Bearbeiten
            Spalten zur Anzeige auswählen
              C
              (max %)
              Si
              (max %)
              Mn
              (max %)
              P
              (max %)
              S
              (max %)
              Nb
              (max %)
              0.18 0.50 1.60 0.020 0.010 0.05
              Parameter vergleichen

              Wählen Sie einen zu vergleichenden Parameter aus

              Vergleich

                Kohlenstoffäquivalent CEV

                Bestimmte Spalten ein-/ausblenden Bearbeiten
                Spalten zur Anzeige auswählen
                  Dicke (mm) 5.00 - 20.00 20.01 - 50.00 50.01 - 150.00
                  CEV
                  (max )
                  0.41 0.43 0.45
                  Parameter vergleichen

                  Wählen Sie einen zu vergleichenden Parameter aus

                  Vergleich

                    Toleranzen

                    Thickness ¾ from EN 10029 Class A.

                    Width and length according to EN 10029.

                    Flatness tolerance 4 mm/m.

                    Surface according to EN 10163-2 Class A subclass 1.

                    Lieferzustand

                    Typically(can be chosen by SSAB).

                    5.00 – 30.00 mm: normalized rolled.

                    30.01 – 150 mm: normalized.

                    Beschichtungen

                    Shot blasted & primed surface is available upon request.

                    Certificates

                    SSAB Multisteel SN provides two different certificates:

                    EN 10204-3.1 for SSAB Multisteel SN.

                    EN 10204-3.1+CE for S355K2/J2/J0/JR+N EN 10025-2.

                    Verarbeitung und andere Empfehlungen

                    Welding:

                    Weldability is excellent with all welding processes. Increased working temperature requirements are less than those of the corresponding strength grades of standard steels. This means easier welding and cost savings under both workshop and site welding conditions.

                    Needed working temperatures for thick plates please consult SSAB Tech Support.

                    Forming:

                    SSAB Multisteel offers better formability properties than standard steels. Successful forming requires that the manufacturer uses good workshop techniques. Worn tools, poor lubrication, scratches on the surface of the steel as well as edge burrs will all reduce forming quality.

                    Guaranteed minimum bending radius for all directions is 1.5 x t up to 30 mm thick plate where t = plate thickness.

                    Heat treatment:

                    Recommendations for stress relieving and normalizing

                    Stress relieving 550 – 600°C (target 580°C)

                    2 minutes/millimeter of thickness, however, 30 minutes minimum. Slow cooling in the furnace.

                    Normalizing 900 – 940°C (target 920°C)

                    1 minute/millimeter of thickness, however, 20 minutes minimum. Cooling in free air.

                    Options:

                    Two options for SSAB Multisteel SN are specified below. In the event that the purchaser does not indicate his wish to implement either of these options, SSAB shall supply in accordance with the basic specification. Option can be implement one at a time, not together.

                    1) According to Norsok M-120/MDS Y05:

                    C max 0.16%

                    CEV max 0.41

                    Thickness range 5.0-50.0mm

                    Y05 will be on the certificate and stamped on the plate

                    Option 1 provides three different certificates:

                    EN 10204-3.1 for SSAB Mutisteel SN

                    EN 10204-3.1+CE for S355K2/J2+N EN 10025-2

                    EN 10204-3.1+CE for S355J0/JR+N EN 10025-2

                    2) Low Si value 0.15 - 0.25 %

                    CEV max 0.41

                    Thickness range 5.0-30.0mm

                    Informationen bezüglich Schweißbarkeit und Verarbeitung finden Sie in den SSAB Broschüren auf www.ssab.com oder kontaktieren Sie die Technische Kundenbetreuung