Docol® 1200M martensitic
More about martensitic steelDownload data sheet
Download data sheet
Docol 1200M is available both as hot rolled and cold rolled. Docol 1200M martensitic steel helps improve crashworthiness and ensure a lightweight design and cost-efficient production methods for the automotive industry. Docol is one of the strongest cold rolled advanced high-strength steels on the market and has become the material of choice for automotive applications such as side impact beams, bumpers and structural components.
Cold rolled / UC: thickness 0.50-2.10 mm, width up to 1527 mm.
Cold rolled / EG: thickness 0.80-1.80 mm, width up to 1200 mm.
Hot rolled / UC: thickness 2.00-4.00 mm, width up to 1440 mm.
Slit strip and cut to length sheets are available upon request.
Grade and coating specific restrictions on available dimensions may occur.
Standard | Coating | Test direction |
Yield strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Elongation A80 (min %) |
Elongation A5 (min %) |
BH2 (min MPa) |
Min. inner bending radius for a 90° bend | |
---|---|---|---|---|---|---|---|---|---|
Docol CR950Y1200T-MS | SSAB | UC, EG | T | 950 - | 1200 - 1400 | 3 | — | 30 | 3.5 x t |
Docol HR900Y1180T-MS | SSAB | UC | L | 900 - 1150 | 1180 - 1400 | 5 | 5 | 30 | — |
The testing of mechanical properties of electrogalvanized products is conducted without coating.
For thicknesses < 3.0 mm, Docol HR900Y1180T-MS can be adapted and certified according to VDA 239-100 upon request.
Coating | C (max %) |
Si (max %) |
Mn (max %) |
P (max %) |
S (max %) |
Al (%) |
Nb+Ti (max %) |
Cr+Mo (max %) |
B (max %) |
Cu (max %) |
|
---|---|---|---|---|---|---|---|---|---|---|---|
Docol CR950Y1200T-MS | UC, EG | 0.14 | 0.40 | 2.00 | 0.020 | 0.010 | From 0.015 | 0.10 | — | — | — |
Docol HR900Y1180T-MS | UC | 0.25 | 0.80 | 2.50 | 0.050 | 0.010 | 0.015 - 2.00 | 0.25 | 1.20 | 0.005 | 0.20 |
Hot rolled (UC): Tolerances in accordance to EN 10051
Cold rolled (UC, EG): Tolerances in accordance to EN 10131.
Customized dimensional and shape tolerances are available upon request.
The following improved flatness tolerances are available for cold rolled products upon request.
Thickness (mm) |
Max height 1) (mm) |
---|---|
0.80 - 0.99 | 8 |
1.00 - 1.39 | 7 |
1.40 - 1.59 | 6 |
1.60 - 1.79 | 5 |
1.80 - 2.10 | 4 |
EG coated martensitic grades are supplied with improved flatness tolerances.
1) Distance from the top surface of the strip normal to flat surface. Measured with a ruler on sheets of mother coil width and minimum length 1200 mm. Cross bow and coil set excluded.
The metal coating options for Docol products include:
Electrogalvanized coating (EG) is applied continuously by electro deposition. The coating consists of zinc (>99%). Electrogalvanized steel is characterized by its excellent surface quality and uniform coating thickness.
Grade specific availability of metal coatings for Docol products is given in the Mechanical properties table (Coating).
Coating type | Coating class | Standard | Coating mass per side, single spot test (g/m2) | Thickness per side informative (µm) |
---|---|---|---|---|
EG | 25/25 | EN 10152 | 12 - | 1.7 - |
EG | 50/50 | EN 10152 | 29 - | 4.1 - |
EG | 75/75 | EN 10152 | 47 - | 6.6 - |
EG | 100/100 | EN 10152 | 65 - | 9.1 - |
Docol metal coated products are available with surface quality for unexposed applications.
In addition to these coating masses, OEM specific coatings and single sided EG coatings are available upon request.
Uncoated (UC): available as oiled.
Electrogalvanized (EG): available as oiled and/or chemically passivated or phosphated.
All surface treatments are in accordance with RoHS directive (2011/65/EU) and do not contain Chromium VI (Cr6+). Surface treatments provide only temporary surface protection during transportation and storage. In order to avoid corrosion damages, care must be taken to keep the products dry during transportation and storage. If they become wet, they must be separated and situated so that they are dried quickly.
For information concerning fabrication, see SSAB´s brochures on www.ssab.com or consult Tech Support.
Appropriate health and safety precautions must be taken when bending, welding, cutting, grinding or otherwise working on the products.
Vous voulez découvrir des applications automobiles uniques, essayer de nouvelles méthodes de production, ou créer des pièces plus légères pour améliorer l'efficacité énergétique, la résistance aux chocs et la durabilité ?
Les clients Docol® peuvent profiter d'un accès 24h sur 24, 7 jours sur 7, à toutes les informations sur le formage, qui peuvent servir à des simulations intégrant des aciers automobiles avancés à haute limite élastique.