General Product Description

Normalized structural steel heavy plate.

SSAB Multisteel SNL is hot rolled structural steel for general steel constructions. SNL = Structural Normalized Low Temperature.

Exceeding the requirements of several standard steel grades, SSAB Multisteel SNL is a versatile structural steel for fabricated products and steel frame structures. Formability and highly consistent quality guarantee fast, uninterrupted production, generating clear savings in the costs of material management.

SSAB Multisteel SNL exceeds several steel standards and is available as six standard steel grades: S355N and S355NL according to EN 10025-3 and S355K2+N, S355J2+N, S355J0+N and S355JR+N according to EN 10025-2.

CE marking:

SSAB Raahe Works is authorized to use the CE marking for structural steels according to EN 10025-2 and EN 10025-3 based on EN 10025-1.

The CE marking is marked on an extra page of inspection certification 3.1.

Dimension Range

SSAB Multisteel SNL is available in thickness of 5.00 - 150.00 mm.

Mechanical Properties

Hide/Show specific columns Edit
Select columns to display
    Thickness
    (mmin)
    Yield strength
    (min MPa)
    Tensile strength
    (MPa)
    Elongation A5
    (min %)
    5.00 - 16.000.197 - 0.6299 355 470 - 630 22
    16.01 - 40.000.6303 - 1.575 345 470 - 630 22
    40.01 - 63.001.575 - 2.480 335 470 - 630 22
    63.01 - 80.002.481 - 3.150 325 470 - 630 21
    80.01 - 100.003.150 - 3.9370 315 470 - 630 21
    100.01 - 150.003.9374 - 5.9055 295 450 - 600 21
    Compare parameters

    Select one parameter to compare

    Comparison

      The mechanical properties are tested transverse to the direction of rolling.

      Impact Properties

      Hide/Show specific columns Edit
      Select columns to display
        Min. impact energy for longitudinal testing,
        Charpy V 10x10 mm test specimens
        SSAB Multisteel SNL 27 J / -50 °C
        EN 10025-3 S355NL 27 J / -50 °C
        EN 10025-3 S355N 40 J / -20 °C
        EN 10025-2 S355K2+N 40 J / -20 °C
        EN 10025-2 S355J2+N 27 J / -20 °C
        EN 10025-2 S355J0+N 27 J / 0 °C
        EN 10025-2 S355JR+N J / °C
        Compare parameters

        Select one parameter to compare

        Comparison

          SSAB Multisteel SNL
          Min. impact energy for longitudinal testing,
          Charpy V 10x10 mm test specimens
          27 J / -50 °C
          EN 10025-3 S355NL
          Min. impact energy for longitudinal testing,
          Charpy V 10x10 mm test specimens
          27 J / -50 °C
          EN 10025-3 S355N
          Min. impact energy for longitudinal testing,
          Charpy V 10x10 mm test specimens
          40 J / -20 °C
          EN 10025-2 S355K2+N
          Min. impact energy for longitudinal testing,
          Charpy V 10x10 mm test specimens
          40 J / -20 °C
          EN 10025-2 S355J2+N
          Min. impact energy for longitudinal testing,
          Charpy V 10x10 mm test specimens
          27 J / -20 °C
          EN 10025-2 S355J0+N
          Min. impact energy for longitudinal testing,
          Charpy V 10x10 mm test specimens
          27 J / 0 °C
          EN 10025-2 S355JR+N
          Min. impact energy for longitudinal testing,
          Charpy V 10x10 mm test specimens
          J / °C

          The impact test is made longitudinal to the rolling direction in compliance with EN 10025-1 and EN 10025-2.

          Chemical Composition (ladle analysis)

          Hide/Show specific columns Edit
          Select columns to display
            C
            (max %)
            Si
            (max %)
            Mn
            (max %)
            P
            (max %)
            S
            (max %)
            Nb
            (max %)
            0.18 0.50 1.60 0.020 0.010 0.05
            Compare parameters

            Select one parameter to compare

            Comparison

              Carbon Equivalent CEV

              Hide/Show specific columns Edit
              Select columns to display
                Thickness (mmin) 5.00 - 63.000.197 - 2.480 63.01 - 150.002.481 - 5.9055
                CEV (max %) 0.43 0.45
                Compare parameters

                Select one parameter to compare

                Comparison

                  Tolerances

                  Thickness ¾ from EN 10029 Class A.

                  Width and length according to EN 10029.

                  Flatness tolerance 4 mm/m.

                  Surface according to EN 10163-2 Class A subclass 1.

                  Delivery Conditions

                  Normalized.

                  Coating

                  Shot blasted & primed surface is available upon request.

                  Certificates

                  SSAB Multisteel SNL provides three different certificates:

                  EN 10204-3.1 to SSAB Multisteel SNL.

                  EN 10204-3.1 +CE to S355NL/N EN 10025-3.

                  EN 10204-3.1 +CE to S355K2/J2/J0/JR+N EN 10025-2.

                  Fabrication and Other Recommendations

                  Welding:

                  Weldability is excellent with all welding processes. Increased working temperature requirements are less than those of the corresponding strength grades of standard steels. This means easier welding and cost savings under both workshop and site welding conditions.

                  Needed working temperatures for thick plates please consult SSAB Tech Support.

                  Forming:

                  SSAB Multisteel offers better formability properties than standard steels. Successful forming requires that the manufacturer uses good workshop techniques. Worn tools, poor lubrication, scratches on the surface of the steel as well as edge burrs will all reduce forming quality.

                  Guaranteed minimum bending radius for all directions is 1.5 x t up to 30 mm thick plate where t = plate thickness.

                  Heat treatment:

                  Recommendations for stress relieving and normalizing

                  Stress relieving 550 – 600°C (target 580°C)

                  2 minutes/millimeter of thickness, however, 30 minutes minimum. Slow cooling in the furnace.

                  Normalizing 900 – 940°C (target 920°C)

                  1 minute/millimeter of thickness, however, 20 minutes minimum. Cooling in free air.

                  For information concerning fabrication, see SSAB´s brochures on www.ssab.com or consult Tech Support.

                  Appropriate health and safety precautions must be taken when bending, welding, cutting, grinding or otherwise working on the products.

                  Contact Information

                  www.ssab.com/contact