General Product Description

Normalized or normalized rolled structural steel heavy plate.

SSAB Multisteel SN is hot rolled structural steel for general steel constructions. SN = Structural Normalized.

Exceeding the requirements of several standard steel grades, SSAB Multisteel SN is a versatile structural steel for fabricated products and steel frame structures. Formability and highly consistent quality guarantee fast, uninterrupted production, generating clear savings in the costs of material management.

SSAB Multisteel SN exceeds several steel standards and is available as four standard steel grades: S355K2+N, S355J2+N, S355J0+N and S355JR+N according to EN 10025-2.

CE marking:

SSAB Raahe Works is authorized to use the CE marking for structural steels according to EN 10025-2 based on EN 10025-1.

The CE marking is marked on an extra page of inspection certification 3.1.

Dimension Range

SSAB Multisteel SN is available in thickness of 5.00 - 150.00 mm.

Mechanical Properties

Hide/Show specific columns Edit
Select columns to display
    Thickness
    (mmin)
    Yield strength
    (min MPa)
    Tensile strength
    (MPa)
    Elongation A5
    (min %)
    5.00 - 16.000.197 - 0.6299 355 470 - 630 21
    16.01 - 40.000.6303 - 1.575 345 470 - 630 21
    40.01 - 63.001.575 - 2.480 335 470 - 630 20
    63.01 - 80.002.481 - 3.150 325 470 - 630 19
    80.01 - 100.003.150 - 3.9370 315 470 - 630 19
    100.01 - 150.003.9374 - 5.9055 295 450 - 600 19
    Compare parameters

    Select one parameter to compare

    Comparison

      The mechanical properties are tested transverse to the direction of rolling.

      Impact Properties

      Hide/Show specific columns Edit
      Select columns to display
        Min. impact energy for longitudinal testing,
        Charpy V 10x10 mm test specimens
        SSAB Multisteel SN 40 J / -20 °C
        EN 10025-2 S355K2+N 40 J / -20 °C
        EN 10025-2 S355J2+N 27 J / -20 °C
        EN 10025-2 S355J0+N 27 J / 0 °C
        Compare parameters

        Select one parameter to compare

        Comparison

          SSAB Multisteel SN
          Min. impact energy for longitudinal testing,
          Charpy V 10x10 mm test specimens
          40 J / -20 °C
          EN 10025-2 S355K2+N
          Min. impact energy for longitudinal testing,
          Charpy V 10x10 mm test specimens
          40 J / -20 °C
          EN 10025-2 S355J2+N
          Min. impact energy for longitudinal testing,
          Charpy V 10x10 mm test specimens
          27 J / -20 °C
          EN 10025-2 S355J0+N
          Min. impact energy for longitudinal testing,
          Charpy V 10x10 mm test specimens
          27 J / 0 °C

          The impact test is made longitudinal to the rolling direction in compliance with EN 10025-1 and EN 10025-2.

          Chemical Composition (ladle analysis)

          Hide/Show specific columns Edit
          Select columns to display
            C
            (max %)
            Si
            (max %)
            Mn
            (max %)
            P
            (max %)
            S
            (max %)
            Nb
            (max %)
            0.18 0.50 1.60 0.020 0.010 0.05
            Compare parameters

            Select one parameter to compare

            Comparison

              Carbon Equivalent CEV

              Hide/Show specific columns Edit
              Select columns to display
                Thickness (mmin) 5.00 - 20.000.197 - 0.7874 20.01 - 50.000.7878 - 1.969 50.01 - 150.001.969 - 5.9055
                CEV (max %) 0.41 0.43 0.45
                Compare parameters

                Select one parameter to compare

                Comparison

                  Tolerances

                  Thickness ¾ from EN 10029 Class A.

                  Width and length according to EN 10029.

                  Flatness tolerance 4 mm/m.

                  Surface according to EN 10163-2 Class A subclass 1.

                  Delivery Conditions

                  Typically(can be chosen by SSAB).

                  5.00 – 30.00 mm: normalized rolled.

                  30.01 – 150 mm: normalized.

                  Coating

                  Shot blasted & primed surface is available upon request.

                  Certificates

                  SSAB Multisteel SN provides two different certificates:

                  EN 10204-3.1 for SSAB Multisteel SN.

                  EN 10204-3.1+CE for S355K2/J2/J0/JR+N EN 10025-2.

                  Fabrication and Other Recommendations

                  Welding:

                  Weldability is excellent with all welding processes. Increased working temperature requirements are less than those of the corresponding strength grades of standard steels. This means easier welding and cost savings under both workshop and site welding conditions.

                  Needed working temperatures for thick plates please consult SSAB Tech Support.

                  Forming:

                  SSAB Multisteel offers better formability properties than standard steels. Successful forming requires that the manufacturer uses good workshop techniques. Worn tools, poor lubrication, scratches on the surface of the steel as well as edge burrs will all reduce forming quality.

                  Guaranteed minimum bending radius for all directions is 1.5 x t up to 30 mm thick plate where t = plate thickness.

                  Heat treatment:

                  Recommendations for stress relieving and normalizing

                  Stress relieving 550 – 600°C (target 580°C)

                  2 minutes/millimeter of thickness, however, 30 minutes minimum. Slow cooling in the furnace.

                  Normalizing 900 – 940°C (target 920°C)

                  1 minute/millimeter of thickness, however, 20 minutes minimum. Cooling in free air.

                  Options:

                  Two options for SSAB Multisteel SN are specified below. In the event that the purchaser does not indicate his wish to implement either of these options, SSAB shall supply in accordance with the basic specification. Option can be implement one at a time, not together.

                  1) According to Norsok M-120/MDS Y05:

                  C max 0.16%

                  CEV max 0.41

                  Thickness range 5.0-50.0mm

                  Y05 will be on the certificate and stamped on the plate

                  Option 1 provides three different certificates:

                  EN 10204-3.1 for SSAB Mutisteel SN

                  EN 10204-3.1+CE for S355K2/J2+N EN 10025-2

                  EN 10204-3.1+CE for S355J0/JR+N EN 10025-2

                  2) Low Si value 0.15 - 0.25 %

                  CEV max 0.41

                  Thickness range 5.0-30.0mm

                  For information concerning fabrication, see SSAB´s brochures on www.ssab.com or consult Tech Support.