GreenCoat Cool

Download data sheet

Select Language

Get datasheet by email
Close

Get datasheet by email

На этом сайте

General Product Description

GreenCoat Cool color coated steel is available in regular gloss. It is used in roofing and features special solar heat reflecting properties that make the surface stay cooler than regular coated surfaces. For buildings that need cooling, this product helps to save energy and increase the thermal comfort. The largest difference in surface temperature between GreenCoat Cool and standard products is achieved for dark colors.

GreenCoat Cool color coated steel offers a coating that is optimized to resist corrosion (RC5). The structured surface helps to protect against mechanical wear and is easy to handle during manufacturing. The reverse side of the sheet is painted with a two-layer grey backside coating.

GreenCoat Cool complies with current REACH regulations and is fully chromate-free.

SSAB’s color coated steels are all manufactured according to EN 10169.

Technical Properties

Hide/Show specific columns Edit
Select columns to display
    Technical Properties Regular
    Gloss 40
    Minimum inner bending radius 1.0 x sheet thickness
    Scratch resistance 35 N
    UV radiation resistance RUV3
    Corrosion resistance 1) RC5
    Stain resistance Excellent
    Highest operating temperature 100 °C
    Coating thickness, nominal (primer + top coat) 40 µm
    Coating structure Structured
    Steel designation 2) S280GD, S320GD, S350GD
    Zinc coating 275 g/m2
    Min steel thickness 2) 0.50 mm
    Steel width 2) 1000 - 1500 mm
    Compare parameters

    Select one parameter to compare

    Comparison

      Technical Properties
      Gloss
      Regular
      40
      Technical Properties
      Minimum inner bending radius
      Regular
      1.0 x sheet thickness
      Technical Properties
      Scratch resistance
      Regular
      35 N
      Technical Properties
      UV radiation resistance
      Regular
      RUV3
      Technical Properties
      Corrosion resistance 1)
      Regular
      RC5
      Technical Properties
      Stain resistance
      Regular
      Excellent
      Technical Properties
      Highest operating temperature
      Regular
      100 °C
      Technical Properties
      Coating thickness, nominal (primer + top coat)
      Regular
      40 µm
      Technical Properties
      Coating structure
      Regular
      Structured
      Technical Properties
      Steel designation 2)
      Regular
      S280GD, S320GD, S350GD
      Technical Properties
      Zinc coating
      Regular
      275 g/m2
      Technical Properties
      Min steel thickness 2)
      Regular
      0.50 mm
      Technical Properties
      Steel width 2)
      Regular
      1000 - 1500 mm

      1) Classification into corrosion resistance categories is based on blistering, delamination and damage on bend of the coating after two years exposure in natural outdoor testing sites as specified in EN 10169.

      2) Maximum steel thickness is 1.5 mm and maximum steel width depends on steel thickness. For other steel dimensions or steel grades please contact SSAB Tech Support.

      Colors

      Below are the colors currently available. Other colors can be agreed upon separately.

      Colors shown in the color table are only indicative. To see the real visual appearance of the product, please order a color sample. Please note also that the same colors between the products may differ.

      For information on thermal properties (solar reflectance index SRI or thermal emittance TE) of available colors, please contact SSAB Tech Support.

      5 Available Colors
      Preview colors
      Close

      Colors

      GreenCoat Cool

      Anthracite Grey

      RR2H8 / SS0087

      Regular

      Mountain Grey

      RR23 / SS0036

      Regular

      Nordic Night Black

      RR33 / SS0015

      Regular

      Acorn Brown

      RR827 / SS0434

      Regular

      Cottage Red

      RR29 / SS0758

      Regular

      Reverse Side Coating

      Unless otherwise specified, the reverse side of the sheet is painted with a two-layer coating to further improve the corrosion resistance of the end product. The coating provides good adhesion properties to many adhesives and foams; nevertheless the compatibility needs to be tested case-specifically.

      Hide/Show specific columns Edit
      Select columns to display
        Technical Properties
        Nominal Coating Thickness (primer + top coat) 12 µm
        Color Grey
        Corrosion Resistance Min CPI3
        Compare parameters

        Select one parameter to compare

        Comparison

          Technical Properties
          Nominal Coating Thickness (primer + top coat)
          12 µm
          Technical Properties
          Color
          Grey
          Technical Properties
          Corrosion Resistance
          Min CPI3

          For easy material identification the reverse side of the sheet is stamped with the GreenCoat logo and the product name. The production date is marked to ease material traceability and can be referred to within the guarantee period. An arrow shows the direction of production to ensure installation in a uniform direction.

          Contact Information