General Product Description

Polyester color coated steel from SSAB offers a wide range of colors inspired by Nordic nature. The typical gloss level is regular gloss, but other glosses are available from request.

Polyester is typically used in profiled applications such as warehouses, agricultural buildings, halls and sheds. Polyester possesses good weather resistance properties (RC3) and offers a smooth surface and a good flexibility when processing.

The reverse side of the sheet is painted with a two-layer grey backside coating.

Polyester complies with current REACH regulations and is fully free of chromates.

SSAB’s color coated steels are all manufactured according to EN 10169.

Technical Properties

Hide/Show specific columns Edit
Select columns to display
    Technical Properties Regular
    Gloss 35
    Minimum inner bending radius 3 x sheet thickness
    Scratch resistance 20 N
    UV radiation resistance RUV2-3
    Corrosion resistance 1) RC3
    Stain resistance Satisfactory
    Highest operating temperature 90 °C
    Fire classification, EN 13501-1 A1 s1 d0
    Coating thickness, nominal (primer + top coat) 25 µm
    Coating structure Smooth
    Steel designation 2) S280GD - S350GD, DX51D
    Zinc coating 275 g/m2
    Min steel thickness 2) 0.42 mm
    Steel width 2) 1000 - 1500 mm
    Compare parameters

    Select one parameter to compare

    Comparison

      Technical Properties
      Gloss
      Regular
      35
      Technical Properties
      Minimum inner bending radius
      Regular
      3 x sheet thickness
      Technical Properties
      Scratch resistance
      Regular
      20 N
      Technical Properties
      UV radiation resistance
      Regular
      RUV2-3
      Technical Properties
      Corrosion resistance 1)
      Regular
      RC3
      Technical Properties
      Stain resistance
      Regular
      Satisfactory
      Technical Properties
      Highest operating temperature
      Regular
      90 °C
      Technical Properties
      Fire classification, EN 13501-1
      Regular
      A1 s1 d0
      Technical Properties
      Coating thickness, nominal (primer + top coat)
      Regular
      25 µm
      Technical Properties
      Coating structure
      Regular
      Smooth
      Technical Properties
      Steel designation 2)
      Regular
      S280GD - S350GD, DX51D
      Technical Properties
      Zinc coating
      Regular
      275 g/m2
      Technical Properties
      Min steel thickness 2)
      Regular
      0.42 mm
      Technical Properties
      Steel width 2)
      Regular
      1000 - 1500 mm

      1) Classification into corrosion resistance categories is based on blistering, delamination and damage on bend of the coating after two years exposure in natural outdoor testing sites as specified in EN 10169.

      2) Maximum steel thickness is 1.5 mm and maximum steel width depends on steel thickness. For other steel dimensions or steel grades please contact SSAB Tech Support.

      Colors

      Below are the colors currently available. Other colors can be agreed upon separately.

      Colors shown in the color table are only indicative. To see the real visual appearance of the product, please order a color sample. Please note also that the same colors between the products may differ.

      35 Available Colors
      Preview colors
      Close

      Colors

      Polyester

      Frost White

      RR106 / SS0009

      Regular

      Nordic White

      RR1H3 / SS0020

      Regular

      Winter White

      RR20 / SS0005

      Regular

      White

      RR--- / SS0010

      Regular

      White

      RR135 / SS0248

      Regular

      White

      RR1G5 / SS0109

      Regular

      White

      RR1G6 / SS----

      Regular

      Fog White

      RR143 / SS----

      Regular

      White

      RR1L4 / SS0078

      Regular

      Limestone Grey

      RR268 / SS0022

      Regular

      Cloud Grey

      RR2B1 / SS----

      Regular

      Pebble Grey

      RR21 / SS0011

      Regular

      Stone Grey

      RR22 / SS0554

      Regular

      Rock Grey

      RR237 / SS0061

      Regular

      Grey

      RR2J9 / SS5036

      Regular

      Anthracite Grey

      RR2H8 / SS0087

      Regular

      Mountain Grey

      RR23 / SS0036

      Regular

      Ridge Grey

      RR2F7 / SS0035

      Regular

      Cliff Grey

      RR288 / SS0455

      Regular

      Slate Grey

      RR2H3 / SS0534

      Regular

      Nordic Night Black

      RR33 / SS0015

      Regular

      Walnut Brown

      RR32 / SS0387

      Regular

      Chestnut Brown

      RR887 / SS0435

      Regular

      Acorn Brown

      RR827 / SS0434

      Regular

      Cottage Red

      RR29 / SS0758

      Regular

      Tile Red

      RR750 / SS0760

      Regular

      Brick Red

      RR7F2 / SS0742

      Regular

      Red

      RR786 / SS5415

      Regular

      Harvest Yellow

      RR24 / SS0189

      Regular

      Silver Fir Green

      RR5J3 / SS0975

      Regular

      Leaf Green

      RR594 / SS0874

      Regular

      Pine Green

      RR11 / SS0830

      Regular

      Lake Blue

      RR35 / SS0558

      Regular

      Metallic Silver

      RR946 / SS----

      Regular

      Metallic

      RR947 / SS----

      Regular

      Note for Metallic colors: To ensure tonal consistency of colors on a single exterior face, all material must come from the same production batch. Also the directionality of surfaces has to be consistent especially when sheets are cut to size.

      Reverse Side Coating

      Unless otherwise specified, the reverse side of the sheet is painted with a two-layer coating to further improve the corrosion resistance of the end product. The coating provides good adhesion properties to many adhesives and foams; nevertheless the compatibility needs to be tested case-specifically.

      Hide/Show specific columns Edit
      Select columns to display
        Technical Properties
        Nominal Coating Thickness (primer + top coat) 12 µm
        Color Grey
        Corrosion Resistance Min CPI3
        Compare parameters

        Select one parameter to compare

        Comparison

          Technical Properties
          Nominal Coating Thickness (primer + top coat)
          12 µm
          Technical Properties
          Color
          Grey
          Technical Properties
          Corrosion Resistance
          Min CPI3

          For easy material identification the reverse side of the sheet is stamped with the SSAB logo and the product name. The production date is marked to ease material traceability and can be referred to within the guarantee period. An arrow shows the direction of production to ensure installation in a uniform direction.

          Double Sided Products

          Polyester is also available as a double sided product. However, different sides of the sheet cannot be mixed due to the possibility of a visual difference. The reverse side may show wider variation in color and gloss.

          Protective Film

          Temporary protective films are available for protection during processing and installation. Protective films are applied on the top side of the Product. Films will be centered to the strip meaning that typically there are small unprotected areas in both edges of the strip. Unprotected area may be cut away if customer so wishes. Joined film strip ends are marked with red tape on the edge of the product.

          Products with protective film should be stored in dry and warm conditions, since the adhesion between protective film and color coating decreases both in high and low temperatures. Humidity changes also the adhesion properties and in worst case leaves the adhesive part of the film on the product surface.

          Adhesion of protective film increases over time, eventually making it difficult to remove the film from the Product’s surface. Due to that, protective film is recommended to be removed from the material as soon as possible, but no later than six months from the manufacturing of the Product or after one month from the end product installation depending on which comes first.

          Protective film decreases friction between coil windings, which creates a high risk of coil collapsing on thin gauge coils. Due to the risk of collapsing, SSAB does not recommend protective films for steel nominal thickness ≤ 0,60 mm. If protective film is essential, following precautions must be taken to minimize the risk of collapsing: Max coil weight < 5 tons and self-supporting coil protection shields must be used in the package.

          Typical protective film thickness is around 45µm, max working temperature +80°C and max and min stripping temperatures +40°C & -10°C.

          Protective film has a good resistance to forming but is susceptible to cuts. When working with material with a protective film, clean tools that do not damage the film, and appropriate methods are to be used. Cutting fluids are not needed because the film protects the material surface and reduces friction. Cutting fluids may also have negative impact on the protective film and its adhesion.

          Protective films can be recycled as plastics, combusted or disposed via the municipal waste management system depending on the local waste management guidelines and regulations.

          Contact Information

          www.ssab.com/contact