General Product Description

Laminate FoodSafe from SSAB is available in white colors with a low gloss smooth surface, but can also be supplied with enhanced antistatic properties to minimize the contamination from airborne particles like dust. 

Laminate FoodSafe has typically a metal coated steel substrate with primer, adhesive and PVC-laminate on top side. Each layer is optimized for performance and processing benefits. 

Laminate FoodSafe offers excellent formability for a wide range of applications including walls, ceilings, doors in cold rooms and deep freezers, as well as refrigerated counters, institutional kitchens and production premises. 

Laminate FoodSafe is a highly durable and wear resistant laminated steel product that is resistant to chemicals and detergents which makes it easy to clean. It is non-toxic and suitable for direct contact with food and fully complies with current EU regulations (EU) No 10/2011, REACH regulations and is fully free of chromates.

The reverse side of the sheet is painted with a two-layer grey backside coating.

SSAB’s color coated steels are all manufactured according to EN 10169.
 

Technical Properties

Hide/Show specific columns Edit
Select columns to display
    Technical Properties
    Gloss 11
    Minimum inner bending radius 1 x sheet thickness
    Scratch resistance 55 N
    Highest operating temperature 60 °C
    Lowest operating temperature -40 °C
    Coating thickness, nominal (primer + top coat) 120 µm
    Primer thickness, nominal 6 µm
    Coating structure Smooth
    Steel designation 1) S250GD-S350GD, DX51D
    Zinc coating 275 g/m2
    Min steel thickness 1) 0.42 mm
    Steel width 1) 1000 - 1400 mm
    Compare parameters

    Select one parameter to compare

    Comparison

      Technical Properties
      Gloss
      11
      Technical Properties
      Minimum inner bending radius
      1 x sheet thickness
      Technical Properties
      Scratch resistance
      55 N
      Technical Properties
      Highest operating temperature
      60 °C
      Technical Properties
      Lowest operating temperature
      -40 °C
      Technical Properties
      Coating thickness, nominal (primer + top coat)
      120 µm
      Technical Properties
      Primer thickness, nominal
      6 µm
      Technical Properties
      Coating structure
      Smooth
      Technical Properties
      Steel designation 1)
      S250GD-S350GD, DX51D
      Technical Properties
      Zinc coating
      275 g/m2
      Technical Properties
      Min steel thickness 1)
      0.42 mm
      Technical Properties
      Steel width 1)
      1000 - 1400 mm

      1) Maximum steel thickness is 1.5 mm and maximum steel width depends on steel thickness. For other steel dimensions or steel grades please contact SSAB Tech Support.

      Colors

      Laminate FoodSafe is available in white colors.

      Reverse Side Coating

      Unless otherwise specified, the reverse side of the sheet is painted with a two-layer coating to further improve the corrosion resistance of the end product. The coating provides good adhesion properties to many adhesives and foams; nevertheless the compatibility needs to be tested case-specifically.

      Hide/Show specific columns Edit
      Select columns to display
        Technical Properties
        Nominal Coating Thickness (primer + top coat) 12 µm
        Color Grey
        Corrosion Resistance Min CPI3
        Compare parameters

        Select one parameter to compare

        Comparison

          Technical Properties
          Nominal Coating Thickness (primer + top coat)
          12 µm
          Technical Properties
          Color
          Grey
          Technical Properties
          Corrosion Resistance
          Min CPI3

          For easy material identification the reverse side of the sheet is stamped with the SSAB logo and the product name. The production date is marked to ease material traceability and can be referred to within the guarantee period. An arrow shows the direction of production to ensure installation in a uniform direction.

          Contact Information