General Product Description

GreenCoat Pural Farm BT color coated steel is available in regular finish. It provides a coating where rapeseed oil and other renewable raw materials are used. SSAB has long experience of Bio-based Technology (BT) in GreenCoat® products.

GreenCoat Pural Farm BT offers the highest level of durability for agricultural buildings. It is made with a two-layer epoxy reverse side coating and used for sandwich panels in insulated and heated buildings e.g. chicken houses. The double-sided GreenCoat Pural Farm BT is used for profiles in non-insulated and cold buildings e.g. cowsheds and open storages.

GreenCoat Pural Farm BT color coated steel offers a coating that is optimized to resist weathering resulting in excellent UV resistance (Ruv4 class), corrosion properties (RC5 class) and gives excellent chemical resistance. It also possesses excellent forming properties. The slightly structured surface helps to protect against mechanical wear and is easy to handle during manufacturing.

The reverse side of the sheet is painted with a two-layer grey backside coating.

GreenCoat Pural Farm BT complies with current REACH regulations and is fully chromate-free.

SSAB’s color coated steels are all manufactured according to EN 10169.

GreenCoat and Pural are trademarks of the SSAB group of companies.

Technical Properties

Hide/Show specific columns Edit
Select columns to display
    Technical Properties Regular
    Gloss 40
    Minimum inner bending radius 1 x sheet thickness
    Scratch resistance 35 N
    UV radiation resistance RUV4
    Corrosion resistance 1) RC5
    Stain resistance Very good
    Chemical resistance Excellent
    Highest operating temperature 100 °C
    Coating thickness, nominal (primer + top coat) 40 µm
    Coating structure Structured
    Steel designation 2) S280GD, S320GD, S350GD
    Zinc coating 275 g/m2
    Min steel thickness 2) 0.50 mm
    Steel width 2) 1000 - 1500 mm
    Compare parameters

    Select one parameter to compare

    Comparison

      Technical Properties
      Gloss
      Regular
      40
      Technical Properties
      Minimum inner bending radius
      Regular
      1 x sheet thickness
      Technical Properties
      Scratch resistance
      Regular
      35 N
      Technical Properties
      UV radiation resistance
      Regular
      RUV4
      Technical Properties
      Corrosion resistance 1)
      Regular
      RC5
      Technical Properties
      Stain resistance
      Regular
      Very good
      Technical Properties
      Chemical resistance
      Regular
      Excellent
      Technical Properties
      Highest operating temperature
      Regular
      100 °C
      Technical Properties
      Coating thickness, nominal (primer + top coat)
      Regular
      40 µm
      Technical Properties
      Coating structure
      Regular
      Structured
      Technical Properties
      Steel designation 2)
      Regular
      S280GD, S320GD, S350GD
      Technical Properties
      Zinc coating
      Regular
      275 g/m2
      Technical Properties
      Min steel thickness 2)
      Regular
      0.50 mm
      Technical Properties
      Steel width 2)
      Regular
      1000 - 1500 mm

      1) Classification into corrosion resistance categories is based on blistering, delamination and damage on bend of the coating after two years exposure in natural outdoor testing sites as specified in EN 10169.

      2) Maximum steel thickness is 1.5 mm and maximum steel width depends on steel thickness. For other steel dimensions or steel grades please contact SSAB Tech Support.

      Colors

      Below are the colors currently available. Other colors can be agreed upon separately.

      Colors shown in the color table are only indicative. To see the real visual appearance of the product, please order a color sample. Please note also that the same colors between the products may differ.

      To ensure tonal consistency of colors on a single exterior face, all material should come from the same production batch. The directionality of surfaces should also be consistent especially when sheets are cut to size.

      13 Available Colors
      Preview colors
      Close

      Colors

      GreenCoat Pural Farm BT

      Stone Grey

      RR22 / SS0554

      Regular

      Rock Grey

      RR237 / SS0061

      Regular

      Mountain Grey

      RR23 / SS0036

      Regular

      Slate Grey

      RR2H3 / SS0534

      Regular

      Nordic Night Black

      RR33 / SS0015

      Regular

      Walnut Brown

      RR32 / SS0387

      Regular

      Chestnut Brown

      RR887 / SS0435

      Regular

      Hazelnut Brown

      RR8H2 / SS0426

      Regular

      Cottage Red

      RR29 / SS0758

      Regular

      Brick Red

      RR7F2 / SS0742

      Regular

      Harvest Yellow

      RR24 / SS0189

      Regular

      Pine Green

      RR11 / SS0830

      Regular

      Lake Blue

      RR35 / SS0558

      Regular

      Reverse Side Coating

      Unless otherwise specified, the reverse side of the sheet is painted with a two-layer coating to further improve the corrosion resistance of the end product. The coating provides good adhesion properties to many adhesives and foams; nevertheless the compatibility needs to be tested case-specifically.

      Hide/Show specific columns Edit
      Select columns to display
        Technical Properties
        Nominal Coating Thickness (primer + top coat) 12 µm
        Color Grey
        Corrosion Resistance Min CPI3
        Compare parameters

        Select one parameter to compare

        Comparison

          Technical Properties
          Nominal Coating Thickness (primer + top coat)
          12 µm
          Technical Properties
          Color
          Grey
          Technical Properties
          Corrosion Resistance
          Min CPI3

          For easy material identification the reverse side of the sheet is stamped with the GreenCoat logo and the product name. The production date is marked to ease material traceability and can be referred to within the guarantee period. An arrow shows the direction of production to ensure installation in a uniform direction.

          Double Sided Products

          GreenCoat Pural Farm BT is also available as a double sided product. However, different sides of the sheet cannot be mixed due to the possibility of a visual difference. The reverse side may show wider variation in color and gloss.

          Contact Information

          www.ssab.com/contact