Rough Matt Polyester

Download data sheet

Select Language

Get datasheet by email
Close

Get datasheet by email

На этом сайте

General Product Description

Rough Matt Polyester color coated steel from SSAB is available in a rough matt finish and offers colors inspired by Nordic nature. 

It has specifically been developed for the use in tiles and other roofing profiles and offers good profiling properties which are reached through a harder surface resulting in a product which is “problem-free” during profiling, transportation and installation. The long-term durability properties are according to SSAB’s high standards.

The reverse side of the sheet is painted with a two-layer grey backside coating.
 
Rough Matt Polyester complies with current REACH regulations and is fully free of chromates.

SSAB’s color coated steels are all manufactured according to EN 10169.

Technical Properties

Hide/Show specific columns Edit
Select columns to display
    Technical Properties Matt
    Gloss 4
    Minimum inner bending radius 2 x sheet thickness
    Scratch resistance 25 N
    UV radiation resistance RUV3
    Corrosion resistance 1) RC4
    Stain resistance Good
    Highest operating temperature 90 °C
    Fire classification, EN 13501-1 A2 s1 d0
    Coating thickness, nominal (primer + top coat) 30 µm
    Coating structure Wrinkled
    Steel designation 2) S280GD, S320GD, S350GD
    Zinc coating 275 g/m2
    Min steel thickness 2) 0.45 mm
    Steel width 2) 1000 - 1300 mm
    Compare parameters

    Select one parameter to compare

    Comparison

      Technical Properties
      Gloss
      Matt
      4
      Technical Properties
      Minimum inner bending radius
      Matt
      2 x sheet thickness
      Technical Properties
      Scratch resistance
      Matt
      25 N
      Technical Properties
      UV radiation resistance
      Matt
      RUV3
      Technical Properties
      Corrosion resistance 1)
      Matt
      RC4
      Technical Properties
      Stain resistance
      Matt
      Good
      Technical Properties
      Highest operating temperature
      Matt
      90 °C
      Technical Properties
      Fire classification, EN 13501-1
      Matt
      A2 s1 d0
      Technical Properties
      Coating thickness, nominal (primer + top coat)
      Matt
      30 µm
      Technical Properties
      Coating structure
      Matt
      Wrinkled
      Technical Properties
      Steel designation 2)
      Matt
      S280GD, S320GD, S350GD
      Technical Properties
      Zinc coating
      Matt
      275 g/m2
      Technical Properties
      Min steel thickness 2)
      Matt
      0.45 mm
      Technical Properties
      Steel width 2)
      Matt
      1000 - 1300 mm

      1) Classification into corrosion resistance categories is based on blistering, delamination and damage on bend of the coating after two years exposure in natural outdoor testing sites as specified in EN 10169.

      2) Maximum steel thickness is 1.5 mm and maximum steel width depends on steel thickness. For other steel dimensions or steel grades please contact SSAB Tech Support.

      Colors

      Below are the colors currently available. Other colors can be agreed upon separately.

      Colors shown in the color table are only indicative. To see the real visual appearance of the product, please order a color sample. Please note also that the same colors between the products may differ.

      8 Available Colors
      Preview colors
      Close

      Colors

      Rough Matt Polyester

      Mountain Grey

      RR23 / SS0036

      Matt

      Slate Grey

      RR2H3 / SS0534

      Matt

      Nordic Night Black

      RR33 / SS0015

      Matt

      Walnut Brown

      RR32 / SS0387

      Matt

      Chestnut Brown

      RR887 / SS0435

      Matt

      Cottage Red

      RR29 / SS0758

      Matt

      Tile Red

      RR750 / SS0760

      Matt

      Pine Green

      RR11 / SS0830

      Matt

      Note for all colors: To ensure tonal consistency of colors on a single exterior face, all material must come from the same production batch. Also the directionality of surfaces has to be consistent especially when sheets are cut to size.

      Reverse Side Coating

      Unless otherwise specified, the reverse side of the sheet is painted with a two-layer coating to further improve the corrosion resistance of the end product. The coating provides good adhesion properties to many adhesives and foams; nevertheless the compatibility needs to be tested case-specifically.

      Hide/Show specific columns Edit
      Select columns to display
        Technical Properties
        Nominal Coating Thickness (primer + top coat) 12 µm
        Color Grey
        Corrosion Resistance Min CPI3
        Compare parameters

        Select one parameter to compare

        Comparison

          Technical Properties
          Nominal Coating Thickness (primer + top coat)
          12 µm
          Technical Properties
          Color
          Grey
          Technical Properties
          Corrosion Resistance
          Min CPI3

          For easy material identification the reverse side of the sheet is stamped with the SSAB logo and the product name. The production date is marked to ease material traceability and can be referred to within the guarantee period. An arrow shows the direction of production to ensure installation in a uniform direction.

          Contact Information

          www.ssab.com/contact