GreenCoat FoodSafe BT

Download data sheet

Select Language

Get datasheet by email
Close

Get datasheet by email

На этом сайте

General Product Description

GreenCoat FoodSafe BT color coated steel is a sustainable food-grade interior product for the food industry’s needs. It meets the demanding requirements of the food industry and can be used on premises where food is handled.

GreenCoat FoodSafe BT offers certified non-toxic, easy to clean and durable color coated steel solutions for walls, ceilings, doors in cold rooms and deep freezers, as well as refrigerated counters, institutional kitchens and production premises.

GreenCoat FoodSafe BT color coated steel provides a coating where rapeseed oil and other renewable raw materials are used. SSAB has long experience of Bio-based Technology (BT) in GreenCoat® products.

GreenCoat FoodSafe BT complies with current EU chemical regulations including: EC No 1272/2008, (EU) No 10/2011 and EU REACH.

The reverse side of the sheet is painted with a two-layer grey backside coating.

GreenCoat FoodSafe BT complies with current REACH regulations and is fully chromate-free.

SSAB’s color coated steels are all manufactured according to EN 10169.

Technical Properties

Hide/Show specific columns Edit
Select columns to display
    Technical Properties Regular
    Gloss 40
    Minimum inner bending radius 1.5 x sheet thickness
    Scratch resistance 30 N
    Highest operating temperature 100 °C
    Lowest operating temperature -30 °C
    Fire classification, EN 13501-1 A2 s1 d0
    Coating thickness, nominal (primer + top coat) 30 µm
    Coating structure Structured
    Steel designation 1) S250GD-S350GD, DX51D
    Zinc coating 275 g/m2
    Min steel thickness 1) 0.50 mm
    Steel width 1) 1000 - 1500 mm
    Compare parameters

    Select one parameter to compare

    Comparison

      Technical Properties
      Gloss
      Regular
      40
      Technical Properties
      Minimum inner bending radius
      Regular
      1.5 x sheet thickness
      Technical Properties
      Scratch resistance
      Regular
      30 N
      Technical Properties
      Highest operating temperature
      Regular
      100 °C
      Technical Properties
      Lowest operating temperature
      Regular
      -30 °C
      Technical Properties
      Fire classification, EN 13501-1
      Regular
      A2 s1 d0
      Technical Properties
      Coating thickness, nominal (primer + top coat)
      Regular
      30 µm
      Technical Properties
      Coating structure
      Regular
      Structured
      Technical Properties
      Steel designation 1)
      Regular
      S250GD-S350GD, DX51D
      Technical Properties
      Zinc coating
      Regular
      275 g/m2
      Technical Properties
      Min steel thickness 1)
      Regular
      0.50 mm
      Technical Properties
      Steel width 1)
      Regular
      1000 - 1500 mm

      1) Maximum steel thickness is 1.5 mm and maximum steel width depends on steel thickness. For other steel dimensions or steel grades please contact SSAB Tech Support.

      Colors

      Below are the colors currently available. Other colors can be agreed upon separately.

      Colors shown in the color table are only indicative. To see the real visual appearance of the product, please order a color sample. Please note also that the same colors between the products may differ.

      1 Available Colors
      Preview colors
      Close

      Colors

      GreenCoat FoodSafe BT

      Antique White

      RR--- / SS0007

      Regular

      Reverse Side Coating

      Unless otherwise specified, the reverse side of the sheet is painted with a two-layer coating to further improve the corrosion resistance of the end product. The coating provides good adhesion properties to many adhesives and foams; nevertheless the compatibility needs to be tested case-specifically.

      Hide/Show specific columns Edit
      Select columns to display
        Technical Properties
        Nominal Coating Thickness (primer + top coat) 12 µm
        Color Grey
        Corrosion Resistance Min CPI3
        Compare parameters

        Select one parameter to compare

        Comparison

          Technical Properties
          Nominal Coating Thickness (primer + top coat)
          12 µm
          Technical Properties
          Color
          Grey
          Technical Properties
          Corrosion Resistance
          Min CPI3

          For easy material identification the reverse side of the sheet is stamped with the GreenCoat logo and the product name. The production date is marked to ease material traceability and can be referred to within the guarantee period. An arrow shows the direction of production to ensure installation in a uniform direction.

          Contact Information

          www.ssab.com/contact