GreenCoat TSP Pural BT

Download data sheet

General Product Description

GreenCoat TSP Pural BT color coated steel is available in matt, metallic and satin finishes and offers a wide range of colors inspired by Nordic nature. It provides a coating where rapeseed oil and other renewable raw materials are used. SSAB has long experience of Bio-based Technology (BT) in GreenCoat® products.

This product has been developed together with tinsmiths in order to obtain optimum product properties combined with Nordic quality steel and an excellent coating. The result is a unique, premium product for tinsmiths.

 

GreenCoat TSP Pural BT offers the highest level of durability for standing-seam systems and can be used in all premium tinsmith applications. The formable TSP (TinSmith Pro) steel has practically no spring back, which allows for very tight folding.

GreenCoat TSP Pural BT color coated steel offers a coating that is optimized to resist weathering, resulting in excellent UV resistance (Ruv5 for matt appearance) and corrosion classes (RC5+). The product has excellent scratch resistance and is easy to handle during manufacturing. GreenCoat TSP Pural BT is highly formable and workable at temperatures down to – 15°C, allowing for year-round installation at lower costs.

 

The newly developed satin appearance of GreenCoat TSP Pural BT responds well to current architectural and design trends. It has a gloss level of 20.


The reverse side of the sheet is painted with a two-layer grey backside coating.

GreenCoat TSP Pural BT complies with current REACH regulations and is fully chromate free.

SSAB’s color coated steels are all manufactured according to EN 10169.

GreenCoat and Pural are trademarks of the SSAB group of companies.

Technical Properties

Technical Properties
Technical Properties
Gloss
Matt
< 5
Metallic
40
Satin
20
Technical Properties
Technical Properties
Minimum inner bending radius
Matt
1 x sheet thickness
Metallic
1 x sheet thickness
Satin
1 x sheet thickness
Technical Properties
Technical Properties
Scratch resistance
Matt
40 N
Metallic
35 N
Satin
40 N
Technical Properties
Technical Properties
Lowest forming temperature
Matt
-15 °C
Metallic
-15 °C
Satin
-15 °C
Technical Properties
Technical Properties
UV radiation resistance
Matt
RUV5
Metallic
RUV4
Satin
RUV4-5
Technical Properties
Technical Properties
Corrosion resistance 1)
Matt
RC5+
Metallic
RC5+
Satin
RC5+
Technical Properties
Technical Properties
Stain resistance
Matt
Very good
Metallic
Very good
Satin
Very good
Technical Properties
Technical Properties
Highest operating temperature
Matt
100 °C
Metallic
100 °C
Satin
100 °C
Technical Properties
Technical Properties
Fire classification, EN 13501-1
Matt
A1 s1 d0
Metallic
A1 s1 d0
Satin
A1 s1 d0
Technical Properties
Technical Properties
Coating thickness, nominal (primer + top coat)
Matt
50 µm
Metallic
45 µm
Satin
50 µm
Technical Properties
Technical Properties
Coating structure
Matt
Structured and wrinkled
Metallic
Smooth
Satin
Structured
Technical Properties
Technical Properties
Steel designation
Matt
TSP 2)
Metallic
TSP 2)
Satin
TSP 2)
Technical Properties
Technical Properties
Yield strength Rp0.2 Typical
Matt
190 MPa
Metallic
190 MPa
Satin
190 MPa
Technical Properties
Technical Properties
Tensile strength Rm Typical
Matt
330 MPa
Metallic
330 MPa
Satin
330 MPa
Technical Properties
Technical Properties
Elongation A80 Typical
Matt
40 %
Metallic
40 %
Satin
40 %
Technical Properties
Technical Properties
Zinc coating
Matt
275 g/m2
Metallic
275 g/m2
Satin
275 g/m2
Technical Properties
Technical Properties
Min steel thickness
Matt
0.60 mm
Metallic
0.60 mm
Satin
0.60 mm
Technical Properties
Technical Properties
Steel width
Matt
1000 - 1500 mm
Metallic
1000 - 1420 mm
Satin
1000 - 1500 mm

1) Classification into corrosion resistance categories is based on blistering, delamination and damage on bend of the coating after four years exposure in natural outdoor testing sites as specified in EN 10169.

2) TSP fulfills the requirements of EN 10346 DX53D.

Colors

Below are the colors currently available. Other colors can be agreed upon separately.

Colors shown in the color table are only indicative. To see the real visual appearance of the product, please order a color sample. Please note also that the same colors between the products may differ.

For information on thermal properties (solar reflectance index SRI or thermal emittance TE) of available colors, please contact SSAB Tech Support.

Note especially for Metallic and all Matt colors: To ensure tonal consistency of colors on a single exterior face, all material must come from the same production batch. Also the directionality of surfaces has to be consistent especially when sheets are cut to size. Compared to solid colors, larger measured color variation between production batches is typical for metallic colors, even if color is visually stable.

Reverse Side Coating

Unless otherwise specified, the reverse side of the sheet is painted with a two-layer coating to further improve the corrosion resistance of the end product. The coating provides good adhesion properties to many adhesives and foams; nevertheless the compatibility needs to be tested case-specifically.

Technical Properties
Technical Properties
Nominal Coating Thickness (primer + top coat)
12 µm
Technical Properties
Technical Properties
Color
Grey
Technical Properties
Technical Properties
Corrosion Resistance
Min CPI3

For easy material identification the reverse side of the sheet is stamped with the GreenCoat logo and the product name. The production date is marked to ease material traceability and can be referred to within the guarantee period. An arrow shows the direction of production to ensure installation in a uniform direction.

Contact Information

www.ssab.com/contact