P200

Download data sheet

Select Language

Get datasheet by email
Close

Get datasheet by email

On this page

General Product Description

SSAB’s Plastisol P200 is a color coated steel that offers a thick coating and an embossed surface. It combines high wear resistance with high durability against corrosion. P200 is easy to process and can be bent without restrictions.

The reverse side of the sheet is painted with a two-layer grey backside coating.
 
P200 complies with current REACH regulations and is fully free of chromates.

SSAB’s color coated steels are all manufactured according to EN 10169.

Technical Properties

Hide/Show specific columns Edit
Select columns to display
    Technical Properties Embossed
    Gloss n/a
    Minimum inner bending radius 0 x sheet thickness
    Scratch resistance 45 N
    UV radiation resistance RUV2
    Corrosion resistance 1) RC5
    Stain resistance Satisfactory
    Highest operating temperature 60 °C
    Fire classification, EN 13501-1 C- s2 d1
    Coating thickness, nominal (primer + top coat) 200 µm
    Coating structure Embossed
    Steel designation 2) S280GD - S350GD, DX51D
    Zinc coating 275 g/m2
    Min steel thickness 2) 0.42 mm
    Steel width 2) 1000 - 1500 mm
    Compare parameters

    Select one parameter to compare

    Comparison

      Technical Properties
      Gloss
      Embossed
      n/a
      Technical Properties
      Minimum inner bending radius
      Embossed
      0 x sheet thickness
      Technical Properties
      Scratch resistance
      Embossed
      45 N
      Technical Properties
      UV radiation resistance
      Embossed
      RUV2
      Technical Properties
      Corrosion resistance 1)
      Embossed
      RC5
      Technical Properties
      Stain resistance
      Embossed
      Satisfactory
      Technical Properties
      Highest operating temperature
      Embossed
      60 °C
      Technical Properties
      Fire classification, EN 13501-1
      Embossed
      C- s2 d1
      Technical Properties
      Coating thickness, nominal (primer + top coat)
      Embossed
      200 µm
      Technical Properties
      Coating structure
      Embossed
      Embossed
      Technical Properties
      Steel designation 2)
      Embossed
      S280GD - S350GD, DX51D
      Technical Properties
      Zinc coating
      Embossed
      275 g/m2
      Technical Properties
      Min steel thickness 2)
      Embossed
      0.42 mm
      Technical Properties
      Steel width 2)
      Embossed
      1000 - 1500 mm

      1) Classification into corrosion resistance categories is based on blistering, delamination and damage on bend of the coating after two years exposure in natural outdoor testing sites as specified in EN 10169.

      2) Maximum steel thickness is 1.5 mm and maximum steel width depends on steel thickness. For other steel dimensions or steel grades please contact SSAB Tech Support.

      Colors

      Below are the colors currently available. Other colors can be agreed upon separately.

      Colors shown in the color table are only indicative. To see the real visual appearance of the product, please order a color sample. Please note also that the same colors between the products may differ.

      4 Available Colors
      Preview colors
      Close

      Colors

      P200

      White

      RR120 / SS----

      Embossed

      Anthracite Grey

      RR2H8 / SS0087

      Embossed

      Nordic Night Black

      RR33 / SS0015

      Embossed

      Walnut Brown

      RR32 / SS0387

      Embossed

      Reverse Side Coating

      Unless otherwise specified, the reverse side of the sheet is painted with a two-layer coating to further improve the corrosion resistance of the end product. The coating provides good adhesion properties to many adhesives and foams; nevertheless the compatibility needs to be tested case-specifically.

      Hide/Show specific columns Edit
      Select columns to display
        Technical Properties
        Nominal Coating Thickness (primer + top coat) 12 µm
        Color Grey
        Corrosion Resistance Min CPI3
        Compare parameters

        Select one parameter to compare

        Comparison

          Technical Properties
          Nominal Coating Thickness (primer + top coat)
          12 µm
          Technical Properties
          Color
          Grey
          Technical Properties
          Corrosion Resistance
          Min CPI3

          For easy material identification the reverse side of the sheet is stamped with the SSAB logo and the product name. The production year is marked to ease material traceability and can be referred to within the guarantee period. An arrow shows the direction of production to ensure installation in a uniform direction.