General Product Description

Polyester Indoor color coated steel from SSAB is available in a smooth surface and offers a wide range of colors and gloss options. 

It is used in e.g. ceilings, load-bearing profiles, doors, window frames, cabinets and interior walls. Polyester Indoor color coated steel is also used in products in metal fabrication and in claddings of the food industry.

Unless otherwise specified, the reverse side of the sheet is painted with a two-layer grey backside coating.
 
Polyester Indoor complies with current REACH regulations and is fully free of chromates.

SSAB’s color coated steels are all manufactured according to EN 10169.

Technical Properties

Hide/Show specific columns Edit
Select columns to display
    Technical Properties
    Gloss 10 - 85
    Minimum inner bending radius, zinc coating 100g/m2 2 x sheet thickness
    Minimum inner bending radius, zinc coating 275g/m2 4 x sheet thickness
    Scratch resistance 20 N
    Highest operating temperature 90 °C
    Fire classification, EN 13501-1 A1 s1 d0
    Coating thickness, nominal (primer + top coat) 25 µm
    Coating structure Smooth
    Steel designation 1) S250GD - S350GD, DX51D
    Zinc coating 100 g/m2, 140 g/m2, 275 g/m2
    Min steel thickness 1) 0.40 mm
    Steel width 1) 1000 - 1424 mm
    Compare parameters

    Select one parameter to compare

    Comparison

      Technical Properties
      Gloss
      10 - 85
      Technical Properties
      Minimum inner bending radius, zinc coating 100g/m2
      2 x sheet thickness
      Technical Properties
      Minimum inner bending radius, zinc coating 275g/m2
      4 x sheet thickness
      Technical Properties
      Scratch resistance
      20 N
      Technical Properties
      Highest operating temperature
      90 °C
      Technical Properties
      Fire classification, EN 13501-1
      A1 s1 d0
      Technical Properties
      Coating thickness, nominal (primer + top coat)
      25 µm
      Technical Properties
      Coating structure
      Smooth
      Technical Properties
      Steel designation 1)
      S250GD - S350GD, DX51D
      Technical Properties
      Zinc coating
      100 g/m2, 140 g/m2, 275 g/m2
      Technical Properties
      Min steel thickness 1)
      0.40 mm
      Technical Properties
      Steel width 1)
      1000 - 1424 mm

      1) Maximum steel thickness is 1.5 mm and maximum steel width depends on steel thickness. For other steel dimensions or steel grades please contact SSAB Tech Support.

      Colors

      Polyester Indoor color coated steel offers a wide range of colors and gloss levels. In special cases, the coating can be matched to customer's requirements.

      Note for Metallic colors: To ensure tonal consistency of colors on a single exterior face, all material must come from the same production batch. Also the directionality of surfaces has to be consistent especially when sheets are cut to size.

      Reverse Side Coating

      Unless otherwise specified, the reverse side of the sheet is painted with a two-layer coating to further improve the corrosion resistance of the end product. The coating provides good adhesion properties to many adhesives and foams; nevertheless the compatibility needs to be tested case-specifically.

      Hide/Show specific columns Edit
      Select columns to display
        Technical Properties
        Nominal Coating Thickness (primer + top coat) 12 µm
        Color Grey
        Corrosion Resistance Min CPI3
        Compare parameters

        Select one parameter to compare

        Comparison

          Technical Properties
          Nominal Coating Thickness (primer + top coat)
          12 µm
          Technical Properties
          Color
          Grey
          Technical Properties
          Corrosion Resistance
          Min CPI3

          For easy material identification the reverse side of the sheet is stamped with the SSAB logo and the product name. The production year is marked to ease material traceability and can be referred to within the guarantee period. An arrow shows the direction of production to ensure installation in a uniform direction.

          Protective Film

          Temporary protective films are available for protection during processing and installation. Protective films are applied on the top side of the Product. Films will be centered to the strip meaning that typically there are small unprotected areas in both edges of the strip. Unprotected area may be cut away if customer so wishes. Joined film strip ends are marked with red tape on the edge of the product.

          Products with protective film should be stored in dry and warm conditions, since the adhesion between protective film and color coating decreases both in high and low temperatures. Humidity changes also the adhesion properties and in worst case leaves the adhesive part of the film on the product surface.

          Adhesion of protective film increases over time, eventually making it difficult to remove the film from the Product’s surface. Due to that, protective film is recommended to be removed from the material as soon as possible, but no later than six months from the manufacturing of the Product or after one month from the end product installation depending on which comes first.

          Protective film decreases friction between coil windings, which creates a high risk of coil collapsing on thin gauge coils. Due to the risk of collapsing, SSAB does not recommend protective films for steel nominal thickness ≤ 0,60 mm. If protective film is essential, following precautions must be taken to minimize the risk of collapsing: Max coil weight < 5 tons and self-supporting coil protection shields must be used in the package.

          Typical protective film thickness is around 45µm, max working temperature +80°C and max and min stripping temperatures +40°C & -10°C.

          Protective film has a good resistance to forming but is susceptible to cuts. When working with material with a protective film, clean tools that do not damage the film, and appropriate methods are to be used. Cutting fluids are not needed because the film protects the material surface and reduces friction. Cutting fluids may also have negative impact on the protective film and its adhesion.

          Protective films can be recycled as plastics, combusted or disposed via the municipal waste management system depending on the local waste management guidelines and regulations.