General Product Description

GreenCoat RWS Pro color coated steel is available in regular finish and offers a wide range of colors inspired by Nordic nature.

GreenCoat RWS Pro offers a high level of durability for rainwater systems using a double-sided coating (same coating is applied on both sides of the sheet).

GreenCoat RWS Pro color coated steel is optimized for weather and wear resistance. It provides good protection against corrosion (RC5) and mechanical abrasion as well as very good gloss retention and color fastness. GreenCoat RWS Pro possesses excellent forming properties enabling very demanding folding even down to -15°C, allowing for year round installation at lower costs.

Excellent weather resistance together with regular maintenance and the cleaning of rainwater systems can maximize the service life of the product.

GreenCoat RWS Pro complies with current REACH regulations and is fully chromate-free.

SSAB’s color coated steels are all manufactured according to EN 10169.

Technical Properties

Hide/Show specific columns Edit
Select columns to display
    Technical Properties Regular
    Gloss 40
    Minimum inner bending radius 0.5 x sheet thickness
    Scratch resistance 30 N
    Lowest forming temperature -15 °C
    UV radiation resistance RUV3
    Corrosion resistance 1) RC5
    Stain resistance Very good
    Highest operating temperature 100 °C
    Coating thickness, nominal (primer + top coat) 35 µm
    Coating structure Structured
    Steel designation 2) FAX, PLX 3)
    Zinc coating 275 g/m2
    Min steel thickness 2) 0.50 mm
    Steel width 2) 1000 - 1500 mm
    Compare parameters

    Select one parameter to compare

    Comparison

      Technical Properties
      Gloss
      Regular
      40
      Technical Properties
      Minimum inner bending radius
      Regular
      0.5 x sheet thickness
      Technical Properties
      Scratch resistance
      Regular
      30 N
      Technical Properties
      Lowest forming temperature
      Regular
      -15 °C
      Technical Properties
      UV radiation resistance
      Regular
      RUV3
      Technical Properties
      Corrosion resistance 1)
      Regular
      RC5
      Technical Properties
      Stain resistance
      Regular
      Very good
      Technical Properties
      Highest operating temperature
      Regular
      100 °C
      Technical Properties
      Coating thickness, nominal (primer + top coat)
      Regular
      35 µm
      Technical Properties
      Coating structure
      Regular
      Structured
      Technical Properties
      Steel designation 2)
      Regular
      FAX, PLX 3)
      Technical Properties
      Zinc coating
      Regular
      275 g/m2
      Technical Properties
      Min steel thickness 2)
      Regular
      0.50 mm
      Technical Properties
      Steel width 2)
      Regular
      1000 - 1500 mm

      1) Classification into corrosion resistance categories is based on blistering, delamination and damage on bend of the coating after two years exposure in natural outdoor testing sites as specified in EN 10169.

      2) Maximum steel thickness is 1.5 mm and maximum steel width depends on steel thickness. For other steel dimensions or steel grades please contact SSAB Tech Support.

      3) FAX fulfills the requirements of EN 10346 DX51D, PLX fulfills the requirements of EN 10346 DX54D.

      Colors

      Below are the colors currently available. Other colors can be agreed upon separately.

      Colors shown in the color table are only indicative. To see the real visual appearance of the product, please order a color sample. Please note also that the same colors between the products may differ.

      18 Available Colors
      Preview colors
      Close

      Colors

      GreenCoat RWS Pro

      Nordic White

      RR1H3 / SS0020

      Regular

      Winter White

      RR20 / SS0005

      Regular

      Snow White

      RR19 / SS0001

      Regular

      Pebble Grey

      RR21 / SS0011

      Regular

      Stone Grey

      RR22 / SS0554

      Regular

      Anthracite Grey

      RR2H8 / SS0087

      Regular

      Mountain Grey

      RR23 / SS0036

      Regular

      Ridge Grey

      RR2F7 / SS0035

      Regular

      Nordic Night Black

      RR33 / SS0015

      Regular

      Walnut Brown

      RR32 / SS0387

      Regular

      Chestnut Brown

      RR887 / SS0435

      Regular

      Acorn Brown

      RR827 / SS0434

      Regular

      Cocoa Brown

      RR8G2 / SS6056

      Regular

      Cottage Red

      RR29 / SS0758

      Regular

      Brick Red

      RR7F2 / SS0742

      Regular

      Pine Green

      RR11 / SS0830

      Regular

      Metallic Silver

      RR40 / SS0045

      Regular

      Metallic Dark Silver

      RR41 / SS0044

      Regular

      The product especially in metallic colors may have slight tonal difference between batches and especially if the time of production differs significantly.

      Reverse Side Coating

      Same coating is applied on both sides of the sheet.

      The technical properties apply for both sides. However, different sides of the sheet cannot be mixed due to the possibility of a visual difference. The reverse side may show wider variation in color and gloss.

      Reverse side stamping is not applicable for double sided products.

      Contact Information

      www.ssab.com/contact