SSAB Multisteel HS

Спецификации

Выберите язык

Get datasheet by email
Закрыть

Get datasheet by email

На этом сайте

Общее описание продукции

Normalized or normalized rolled structural steel heavy plate. SSAB Multisteel HSD and HSE are hot rolled hull structural steel for general marine steel constructions. HS = Hull Structural – D and E = impact strength class.

Exceeding the requirements of several classification societies rules, SSAB Multisteel HS is a versatile structural steel for shipbuilding. Formability and highly consistent quality guarantee fast, uninterrupted production, generating clear savings in the costs of material management.

SSAB Multisteel HS exceeds several steel standards and is available as six societies rules: DNV (NV), Lloyd's Register EMEA (LR), American Bureau of Shipping (AB), Bureau Veritas (BV), Registro Italiano Navale (RINA), Russian Maritime Register of Shipping (PC) and also possible to certify to EN 10025-2 S355K2+N.

Maximum four (4) different grade if one of them is AB. Otherwise maximum three (3) grades in one plate. Combinations e.g NVD36/ABDH36N/BVDH36/PCD36 or NV D36/BV DH36/S355K2+N. Please enquire for suitable combination before placing the order.

CE marking:

SSAB Raahe Works is authorized to use the CE marking for structural steels according to EN 10025-1 and EN 10025-2. The CE marking is marked on an extra page of inspection certification 3.1 for S355K2+N. CE marking can be given only if S355K2+N is one of the steel grades in the combination.

Типоразмерный ряд

SSAB Multisteel HSD is available in thicknesses of 5.00 - 150.00 mm.

SSAB Multisteel HSE is available in thicknesses of 5.00 - 150.00 mm.

(If PC is involved in the combination max thickness is 100 mm.)

Механические свойства

Скрыть/показать определённые столбцы Редактировать
Выбрать столбцы для отображения
    Толщина
    (ммin)
    Предел текучести
    (мин МПа)
    Tensile strength
    (МПа)
    Относительное удлинение A5
    (min %)
    5.00 - 100.000.197 - 3.9370 355 490 - 620 21
    100.00 - 150.003.9370 - 5.9055 355 490 - 600 21
    Сравнение параметров

    Выберите один параметр для сравнения

    Сравнение

      The mechanical properties are tested transverse to the direction of rolling.

      Ударная вязкость

      Скрыть/показать определённые столбцы Редактировать
      Выбрать столбцы для отображения
        Толщина
        (ммin)
        Мин. работа удара для продольных образцов Шарпи 10 x 10 мм с V- образным надрезом
        SSAB Multisteel HSD 5.00 - 50.000.197 - 1.969 34 J / -20 °C
        50.01 - 70.001.969 - 2.756 41 J / -20 °C
        70.01 - 150.002.756 - 5.9055 50 J / -20 °C
        SSAB Multisteel HSE 5.00 - 50.000.197 - 1.969 34 J / -40 °C
        50.01 - 70.001.969 - 2.756 41 J / -40 °C
        70.01 - 150.002.756 - 5.9055 50 J / -40 °C
        EN 10025-2 S355K2+N 5.00 - 150.000.197 - 5.9055 40 J / -20 °C
        Сравнение параметров

        Выберите один параметр для сравнения

        Сравнение

          The impact test is made longitudinally to the rolling direction in compliance with society rules and EN 10025-2.

          Химический состав (ковшевая проба)

          Скрыть/показать определённые столбцы Редактировать
          Выбрать столбцы для отображения
            C
            (max %)
            Si
            (max %)
            Mn
            (max %)
            P
            (max %)
            S
            (max %)
            Nb
            (max %)
            0.18 0.50 1.60 0.025 0.020 0.05
            Сравнение параметров

            Выберите один параметр для сравнения

            Сравнение

              Углеродный эквивалент CEV

              Скрыть/показать определённые столбцы Редактировать
              Выбрать столбцы для отображения
                тип продукт If only hull structural steel If only hull structural steel If S355K2+N is in the combination If S355K2+N is in the combination
                Толщина (ммin) 5.00 - 60.000.197 - 2.362 60.01 - 150.002.363 - 5.9055 5.00 - 60.000.197 - 2.362 60.01 - 150.002.363 - 5.9055
                CEV (Макс %) 0.45 0.49 0.45 0.47
                Сравнение параметров

                Выберите один параметр для сравнения

                Сравнение

                  Допуски

                  All tolerances according to society rules and EN 10029 – thickness ¾ class B.

                  Flatness tolerance 6 mm/m.

                  Surface according to EN 10163-2 Class A subclass 1 or 3 (when RINA or when thickness is over 100 mm).

                  Условия поставки

                  SSAB Multisteel HSD

                  Typically (can be chosen by SSAB)

                  Normalized rolled (thickness 5.00 - 40.00 mm)

                  Normalized (thickness 40.01 - 150.00 mm)

                  SSAB Multisteel HSE

                  Normalized (thickness 5.00 - 150.00 mm)

                  Coating

                  Shot blasted & primed surface is available upon request.

                  Certificates

                  Mill sheet for hull structural steel according to Classification Society grades.

                  EN 10204-3.1+CE for S355K2+N EN 10025-2 (if chosen to be in the combination).

                  Рекомендации по обработке

                  Welding:

                  Weldability is excellent with all welding processes. Increased working temperature requirements are less than those of the corresponding strength grades of standard steels. This means easier welding and cost savings under both workshop and site welding conditions.

                  Needed working temperatures for thick plates please consult SSAB Tech Support.

                  Forming:

                  SSAB Multisteel offers better formability properties than standard steels. Successful forming requires that the manufacturer uses good workshop techniques. Worn tools, poor lubrication, scratches on the surface of the steel as well as edge burrs will all reduce forming quality.

                  Guaranteed minimum bending radius for all directions is 2 x t up to 30 mm thick plate where t = plate thickness.

                  Heat treatment:

                  Recommendations for stress relieving and normalizing.

                  Stress relieving 550 – 600°C (target 580°C)

                  2 minutes/millimeter of thickness, however, 30 minutes minimum. Slow cooling in the furnace.

                  Normalizing 900 – 940°C (target 920°C)

                  1 minute/millimeter of thickness, however, 20 minutes minimum. Cooling in free air.

                  Информацию об обработке можно найти в брошюрах SSAB на сайте www.ssab.com или связаться с технической поддержкой.

                  Необходимо соблюдать меры предосторожности при гибке, сварке, резке, шлифовании и других механических обработках.

                  Контактные данные

                  www.ssab.com/contact