Docol® PHS 1500 press hardening

Download data sheet

General Product Description

Hardenable boron steel for the automotive industry. Available as both hot rolled and cold rolled. Docol PHS 1500 steels are specially developed for parts and components that are manufactured by direct or indirect hot stamping. Applications include safety parts such as door impact beams, bumper systems and B- pillar reinforcements.

Dimension Range

Cold rolled / UC: thickness 0.70-3.00 mm, width up to 1500 mm.

Hot rolled / UC: thickness 2.00-12.00 mm, width up to 1600 mm.

Slit strip and cut to length sheets are available upon request.

Mechanical Properties

Docol PHS FH 1500

Standard
SSAB
Condition
Full Hard
Test direction
T
Typical yield strength Rp0.2 (MPa)
960
Typical tensile strength Rm (MPa)
1060
Typical elongation A80
(%)
4
Typical elongation A5
(%)
—

Docol PHS CR 1500

Docol PHS HR 1500+A

Standard
SSAB
Condition
Annealed
Test direction
T
Typical yield strength Rp0.2 (MPa)
350 2)
Typical tensile strength Rm (MPa)
530
Typical elongation A80
(%)
25
Typical elongation A5
(%)
33

1) Properties depend on the process.

2) ReH is used instead of Rp0.2.

Chemical Composition (ladle analysis)

C
(%)
C
(%)
0.20 - 0.25
Si
(%)
0.15 - 0.35
Mn
(%)
1.00 - 1.35
P
(max %)
0.025
S
(max %)
0.005
Cr
(max %)
0.35
B
(%)
0.0020 - 0.0050

Tolerances

Cold rolled (UC): Tolerances in accordance to EN 10131.

Hot rolled (UC): Tolerances in accordance to EN 10051.

Customized dimensional and shape tolerances are available upon request.

Surface Treatments

Uncoated (UC): available as oiled.

All surface treatments are in accordance with RoHS directive (2011/65/EU) and do not contain Chromium VI (Cr6+). Surface treatments provide only temporary surface protection during transportation and storage. In order to avoid corrosion damages, care must be taken to keep the products dry during transportation and storage. If they become wet, they must be separated and situated so that they are dried quickly.

Fabrication and Other Recommendations

For information concerning fabrication, see SSAB´s brochures on www.ssab.com or consult Tech Support.

Appropriate health and safety precautions must be taken when bending, welding, cutting, grinding or otherwise working on the products.

Docol® PHS steel product offer

Docol® PHS 1500 press hardening

Visualizza prodotto

Docol® PHS 1800 press hardening

Visualizza prodotto

Docol® PHS 2000 press hardening

Visualizza prodotto

Contenuti correlati

Stock di materiale di prova

Vuoi scoprire applicazioni automotive uniche nel loro genere, sperimentare nuovi metodi di produzione o creare componenti più leggeri che possano migliorare l'efficienza del carburante, la resistenza all'impatto dei veicoli e la sostenibilità?

Per saperne di più

Dati di formatura per gli acciai AHSS Docol®

Gli attuali clienti Docol® hanno accesso 24 ore su 24, 7 giorni su 7 ai dati di formatura necessari per aiutarli nella scelta e nella simulazione degli acciai altoresistenziali di nuova generazione per il settore automobilistico.

Per saperne di più