High reliability high versatility

SSAB Domex® comes as hot rolled plate, hot or cold rolled strip, tubes and sections. It’s also available in different metal-coated grades for corrosion resistance with zinc, galfan and galvannealed coatings.

Contact sales
On this page

Hot rolled plate

Hide/Show specific columns Edit
Select columns to display
    Product Name Dimensions Standards Datasheet
    SSAB Domex 355ML T: 6.00 - 63.00 mm
    W: Up to 3300 mm
    T: 0.236 - 2.480 in
    W: Up to 129.9 in
    EN 10025-4

    SSAB Domex 355ML

    SSAB Domex 420ML T: 8.00 - 63.00 mm
    W: Up to 3300 mm
    T: 0.315 - 2.480 in
    W: Up to 129.9 in
    EN 10025-4

    SSAB Domex 420ML

    SSAB Domex 460ML T: 8.00 - 63.00 mm
    W: Up to 3300 mm
    T: 0.315 - 2.480 in
    W: Up to 129.9 in
    EN 10025-4

    SSAB Domex 460ML

    SSAB Domex 500ML T: 8.00 - 60.00 mm
    W: Up to 3300 mm
    T: 0.315 - 2.362 in
    W: Up to 129.9 in
    SSAB

    SSAB Domex 500ML

    Compare parameters

    Select one parameter to compare

    Comparison

      Hot rolled strip

      Hide/Show specific columns Edit
      Select columns to display
        Product Name Dimensions Standards Datasheet
        SSAB Domex 240YP T: 1.80 - 20.00 mm
        W: Up to 1860 mm
        T: 0.0709 - 0.7874 in
        W: Up to 73.23 in
        EN 10025-2

        SSAB Domex 240YP

        SSAB Domex 315MC T: 1.80 - 18.00 mm
        W: Up to 1860 mm
        T: 0.0709 - 0.7087 in
        W: Up to 73.23 in
        EN 10149-2

        SSAB Domex 315MC

        SSAB Domex 355MC T: 1.80 - 16.00 mm
        W: Up to 1860 mm
        T: 0.0709 - 0.6299 in
        W: Up to 73.23 in
        EN 10149-2

        SSAB Domex 355MC

        SSAB Domex 420MC T: 1.80 - 15.00 mm
        W: Up to 1800 mm
        T: 0.0709 - 0.5906 in
        W: Up to 70.87 in
        EN 10149-2

        SSAB Domex 420MC

        SSAB Domex 460MC T: 2.00 - 13.00 mm
        W: Up to 1800 mm
        T: 0.0787 - 0.5118 in
        W: Up to 70.87 in
        EN 10149-2

        SSAB Domex 460MC

        SSAB Domex 500MC T: 2.00 - 13.00 mm
        W: Up to 1800 mm
        T: 0.0787 - 0.5118 in
        W: Up to 70.87 in
        EN 10149-2

        SSAB Domex 500MC

        SSAB Domex 550MC T: 2.00 - 12.80 mm
        W: Up to 1640 mm
        T: 0.0787 - 0.5039 in
        W: Up to 64.57 in
        EN 10149-2

        SSAB Domex 550MC

        SSAB Domex 355MC Plus T: 3.00 - 12.00 mm
        W: Up to 1860 mm
        T: 0.118 - 0.4724 in
        W: Up to 73.23 in
        EN 10149-2

        SSAB Domex 355MC Plus

        SSAB Domex 420MC Plus T: 3.00 - 10.00 mm
        W: Up to 1860 mm
        T: 0.118 - 0.3937 in
        W: Up to 73.23 in
        EN 10149-2

        SSAB Domex 420MC Plus

        SSAB Domex 460MC Plus T: 4.00 - 10.00 mm
        W: Up to 1800 mm
        T: 0.157 - 0.3937 in
        W: Up to 70.87 in
        EN 10149-2

        SSAB Domex 460MC Plus

        SSAB Domex 500MC Plus T: 3.00 - 8.00 mm
        W: Up to 1800 mm
        T: 0.118 - 0.315 in
        W: Up to 70.87 in
        EN 10149-2

        SSAB Domex 500MC Plus

        Compare parameters

        Select one parameter to compare

        Comparison

          Cold rolled strip

          Hide/Show specific columns Edit
          Select columns to display
            Product Name Dimensions Standards Datasheet
            SSAB Domex 220LA T: 0.40 - 3.00 mm
            W: Up to 1500 mm
            T: 0.016 - 0.118 in
            W: Up to 59.06 in
            SSAB

            SSAB Domex 220LA

            SSAB Domex 260LA T: 0.40 - 3.00 mm
            W: Up to 1500 mm
            T: 0.016 - 0.118 in
            W: Up to 59.06 in
            EN 10268

            SSAB Domex 260LA

            SSAB Domex 280LA T: 0.40 - 3.00 mm
            W: Up to 1500 mm
            T: 0.016 - 0.118 in
            W: Up to 59.06 in
            SSAB

            SSAB Domex 280LA

            SSAB Domex 300LA T: 0.40 - 3.00 mm
            W: Up to 1500 mm
            T: 0.016 - 0.118 in
            W: Up to 59.06 in
            EN 10268

            SSAB Domex 300LA

            SSAB Domex 340LA T: 0.40 - 3.00 mm
            W: Up to 1500 mm
            T: 0.016 - 0.118 in
            W: Up to 59.06 in
            EN 10268

            SSAB Domex 340LA

            SSAB Domex 350LA T: 0.45 - 3.00 mm
            W: Up to 1500 mm
            T: 0.018 - 0.118 in
            W: Up to 59.06 in
            SSAB

            SSAB Domex 350LA

            SSAB Domex 380LA T: 0.45 - 3.00 mm
            W: Up to 1500 mm
            T: 0.018 - 0.118 in
            W: Up to 59.06 in
            EN 10268

            SSAB Domex 380LA

            SSAB Domex 420LA T: 0.50 - 3.00 mm
            W: Up to 1500 mm
            T: 0.020 - 0.118 in
            W: Up to 59.06 in
            EN 10268

            SSAB Domex 420LA

            SSAB Domex 460LA T: 0.50 - 1.60 mm
            W: Up to 1500 mm
            T: 0.020 - 0.0630 in
            W: Up to 59.06 in
            EN 10268

            SSAB Domex 460LA

            SSAB Domex 500LA T: 0.50 - 3.00 mm
            W: Up to 1500 mm
            T: 0.020 - 0.118 in
            W: Up to 59.06 in
            EN 10268

            SSAB Domex 500LA

            Compare parameters

            Select one parameter to compare

            Comparison

              Metal-coated strip

              Hide/Show specific columns Edit
              Select columns to display
                Product Name Dimensions Standards Datasheet
                SSAB Domex 220LAD T: 0.50 - 3.00 mm
                W: Up to 1520 mm
                T: 0.020 - 0.118 in
                W: Up to 59.84 in
                SSAB

                SSAB Domex 220LAD

                SSAB Domex 260LAD T: 0.50 - 3.00 mm
                W: Up to 1520 mm
                T: 0.020 - 0.118 in
                W: Up to 59.84 in
                EN 10346

                SSAB Domex 260LAD

                SSAB Domex 300LAD T: 0.50 - 3.00 mm
                W: Up to 1520 mm
                T: 0.020 - 0.118 in
                W: Up to 59.84 in
                EN 10346

                SSAB Domex 300LAD

                SSAB Domex 340LAD T: 0.50 - 3.00 mm
                W: Up to 1520 mm
                T: 0.020 - 0.118 in
                W: Up to 59.84 in
                EN 10346

                SSAB Domex 340LAD

                SSAB Domex 380LAD T: 0.50 - 3.00 mm
                W: Up to 1520 mm
                T: 0.020 - 0.118 in
                W: Up to 59.84 in
                EN 10346

                SSAB Domex 380LAD

                SSAB Domex 420LAD T: 0.50 - 2.50 mm
                W: Up to 1520 mm
                T: 0.020 - 0.0984 in
                W: Up to 59.84 in
                EN 10346

                SSAB Domex 420LAD

                SSAB Domex 460LAD T: 0.80 - 2.00 mm
                W: Up to 1500 mm
                T: 0.031 - 0.0787 in
                W: Up to 59.06 in
                EN 10346

                SSAB Domex 460LAD

                SSAB Domex 500LAD T: 0.80 - 2.00 mm
                W: Up to 1410 mm
                T: 0.031 - 0.0787 in
                W: Up to 55.51 in
                EN 10346

                SSAB Domex 500LAD

                SSAB Domex 220GD T: 0.45 - 3.00 mm
                W: Up to 1520 mm
                T: 0.018 - 0.118 in
                W: Up to 59.84 in
                EN 10346

                SSAB Domex 220GD

                SSAB Domex 250GD T: 0.45 - 3.00 mm
                W: Up to 1520 mm
                T: 0.018 - 0.118 in
                W: Up to 59.84 in
                EN 10346

                SSAB Domex 250GD

                SSAB Domex 280GD T: 0.45 - 3.00 mm
                W: Up to 1520 mm
                T: 0.018 - 0.118 in
                W: Up to 59.84 in
                EN 10346

                SSAB Domex 280GD

                SSAB Domex 320GD T: 0.50 - 3.00 mm
                W: Up to 1520 mm
                T: 0.020 - 0.118 in
                W: Up to 59.84 in
                EN 10346

                SSAB Domex 320GD

                SSAB Domex 350GD T: 0.50 - 3.00 mm
                W: Up to 1520 mm
                T: 0.020 - 0.118 in
                W: Up to 59.84 in
                EN 10346

                SSAB Domex 350GD

                Compare parameters

                Select one parameter to compare

                Comparison

                  Tubes and sections

                  Hide/Show specific columns Edit
                  Select columns to display
                    Product Name Dimensions Standards Datasheet
                    SSAB Domex Tube 460MH Circular: 42.4 - 323.9 mm
                    Square: 40x40 - 300x300 mm
                    Rectangular: 50x30 - 400x200 mm
                    Wall Thickness: 2.0 - 12.5 mm
                    Circular: 1.67 - 12.75 in
                    Square: in
                    Rectangular: in
                    Wall Thickness: 0.079 - 0.492 in
                    EN 10219-1, EN 10219-2
                    SSAB Domex Tube 500MH Circular: 42.4 - 323.9 mm
                    Square: 40x40 - 300x300 mm
                    Rectangular: 50x30 - 400x200 mm
                    Wall Thickness: 2.0 - 12.5 mm
                    Circular: 1.67 - 12.75 in
                    Square: in
                    Rectangular: in
                    Wall Thickness: 0.079 - 0.492 in
                    EN 10219-2, EN 1090-2
                    SSAB Domex Tube 550MH Circular: 42.4 - 323.9 mm
                    Square: 40x40 - 300x300 mm
                    Rectangular: 50x30 - 400x200 mm
                    Wall Thickness: 2.0 - 12.50 mm
                    Circular: 1.67 - 12.75 in
                    Square: in
                    Rectangular: in
                    Wall Thickness: 0.079 - 0.4921 in
                    EN 10219-2, EN 1090-2
                    SSAB Domex Tube Double Grade Circular: 42.4 - 323.9 mm
                    Square: 40x40 - 300x300 mm
                    Rectangular: 50x30 - 400x200 mm
                    Wall Thickness: 2.0 - 12.50 mm
                    Circular: 1.67 - 12.75 in
                    Square: in
                    Rectangular: in
                    Wall Thickness: 0.079 - 0.4921 in
                    EN 10219-1, EN 10219-2
                    Circular: 42.4 - 323.9 mm
                    Square: 40x40 - 300x300 mm
                    Rectangular: 50x30 - 400x200 mm
                    Wall Thickness: 2.0 - 12.50 mm
                    Circular: 1.67 - 12.75 in
                    Square: in
                    Rectangular: in
                    Wall Thickness: 0.079 - 0.4921 in
                    EN 10219-1, EN 10219-2
                    SSAB Domex Tube 355J2H Circular: 42.4 - 323.9 mm
                    Square: 40x40 - 300x300 mm
                    Rectangular: 50x30 - 400x200 mm
                    Wall Thickness: 2.0 - 12.5 mm
                    Circular: 1.67 - 12.75 in
                    Square: in
                    Rectangular: in
                    Wall Thickness: 0.079 - 0.492 in
                    EN 10219-1, EN 10219-2
                    Compare parameters

                    Select one parameter to compare

                    Comparison