Duroxite® Pipe products are used for transporting slurry and other abrasive fluids that create sliding wear, for example in dredging. The pipes are made with a chromium-rich hardfacing layer deposited inside a mild steel pipe.
Chromium carbide overlay
Typical application: Sliding wear
Shapes: Straight or curved pipes, square-to-round transitions, elbows, T or Y-shaped segments
Diameter: 50-900 mm
Length: 0.9-6.0 mm
Typical surface hardness (double passes): 59-62 HRC
Complex carbide overlay
Typical application: Severe sliding wear
Shapes: Straight or curved pipes, square-to-round transitions, elbows, T or Y-shaped segments
Diameter: 50-900 mm
Length: 0.9-6.0 mm
Typical surface hardness (double passes): 60-65 HRC